Final Magnetic Moment0.428 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-1.668 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.665 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.80 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCaWO4 + W |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCm [8] |
HallC 2y |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 222.4 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 148.3 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 222.4 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 296.5 |
KCl (mp-23193) | <1 1 0> | <1 0 1> | 175.8 |
TePb (mp-19717) | <1 0 0> | <1 0 1> | 175.8 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 296.5 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 222.4 |
GaSe (mp-1943) | <0 0 1> | <1 0 1> | 175.8 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 222.4 |
BN (mp-984) | <0 0 1> | <0 0 1> | 148.3 |
BN (mp-984) | <1 1 0> | <0 0 1> | 296.5 |
MoS2 (mp-1434) | <0 0 1> | <1 0 1> | 175.8 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 1> | 175.8 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 0> | 145.1 |
Al (mp-134) | <1 1 1> | <0 0 1> | 222.4 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 296.5 |
CdTe (mp-406) | <1 0 0> | <1 0 1> | 175.8 |
TiO2 (mp-2657) | <1 1 1> | <1 0 1> | 175.8 |
TiO2 (mp-2657) | <1 1 0> | <1 0 1> | 175.8 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 148.3 |
InSb (mp-20012) | <1 0 0> | <1 0 1> | 175.8 |
BaTiO3 (mp-5986) | <1 0 1> | <0 0 1> | 296.5 |
GdScO3 (mp-5690) | <0 1 1> | <0 0 1> | 222.4 |
GdScO3 (mp-5690) | <1 0 1> | <0 0 1> | 222.4 |
Mg (mp-153) | <0 0 1> | <1 0 1> | 175.8 |
TbScO3 (mp-31119) | <1 0 1> | <0 0 1> | 222.4 |
SiC (mp-11714) | <1 0 1> | <0 0 1> | 296.5 |
Si (mp-149) | <1 1 1> | <0 0 1> | 148.3 |
WS2 (mp-224) | <0 0 1> | <1 0 1> | 175.8 |
C (mp-48) | <0 0 1> | <0 0 1> | 74.1 |
CsI (mp-614603) | <1 1 1> | <0 0 1> | 222.4 |
MgF2 (mp-1249) | <0 0 1> | <1 0 1> | 175.8 |
MgF2 (mp-1249) | <1 1 0> | <1 0 0> | 145.1 |
ZnO (mp-2133) | <0 0 1> | <0 0 1> | 74.1 |
ZnO (mp-2133) | <1 0 0> | <1 0 1> | 175.8 |
SrTiO3 (mp-4651) | <1 0 1> | <0 0 1> | 222.4 |
MgAl2O4 (mp-3536) | <1 1 1> | <0 0 1> | 222.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ca(AgO2)2 (mvc-5243) | 0.1897 | 0.235 | 3 |
Al2NiO4 (mp-705646) | 0.1850 | 0.010 | 3 |
Al2NiO4 (mp-705593) | 0.1844 | 0.199 | 3 |
Al2NiO4 (mp-705610) | 0.1896 | 0.010 | 3 |
LiFe5O8 (mp-706252) | 0.1925 | 0.645 | 3 |
Li2Fe3NiO8 (mp-774943) | 0.1655 | 0.088 | 4 |
Li5Mn2Fe17O32 (mp-777733) | 0.1836 | 0.065 | 4 |
Li2Fe3WO8 (mp-775493) | 0.1889 | 0.048 | 4 |
Li4Co3Sn5O16 (mp-772511) | 0.1957 | 0.026 | 4 |
Li4Mn5Sn3O16 (mp-771907) | 0.1886 | 0.057 | 4 |
Fe3O4 (mp-715491) | 0.3158 | 0.017 | 2 |
Fe3O4 (mp-542433) | 0.3310 | 0.075 | 2 |
Fe3O4 (mp-650112) | 0.2775 | 0.060 | 2 |
Fe3O4 (mp-31770) | 0.3294 | 0.017 | 2 |
Fe3O4 (mp-716052) | 0.3251 | 0.781 | 2 |
Li4Ti3V3(SnO8)2 (mp-780025) | 0.2013 | 0.030 | 5 |
Li4V3Ni3(SbO8)2 (mp-767203) | 0.2155 | 0.026 | 5 |
Li4Ti3Fe3(SbO8)2 (mp-865132) | 0.2186 | 0.257 | 5 |
TaTi9Al3Zn23O48 (mp-686614) | 0.2072 | 0.055 | 5 |
TaTi9Al3Zn23O48 (mp-695545) | 0.1819 | 0.054 | 5 |
Li3MnFeCo(PO4)3 (mp-764931) | 0.6691 | 0.017 | 6 |
Li3MnFeCo(PO4)3 (mp-764809) | 0.6535 | 0.014 | 6 |
Li3MnFeCo(PO4)3 (mp-764869) | 0.6633 | 0.032 | 6 |
Li3MnFeCo(PO4)3 (mp-764969) | 0.6665 | 0.057 | 6 |
Li3MnFeCo(PO4)3 (mp-764870) | 0.6694 | 0.466 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesW: 6.2 eV |
PseudopotentialsVASP PAW: Ca_sv W_pv O |
Final Energy/Atom-6.8399 eV |
Corrected Energy-475.1261 eV
-475.1261 eV = -383.0368 eV (uncorrected energy) - 69.6160 eV (MP Advanced Correction) - 22.4733 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)