Final Magnetic Moment3.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-1.574 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.246 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.11 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMnO2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCm [8] |
HallC 2y |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 177.3 |
CdS (mp-672) | <1 0 1> | <0 1 1> | 196.7 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 177.3 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 59.1 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 177.3 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 177.3 |
BN (mp-984) | <0 0 1> | <0 0 1> | 236.5 |
LiNbO3 (mp-3731) | <1 0 1> | <0 0 1> | 236.5 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 232.1 |
C (mp-66) | <1 1 0> | <0 0 1> | 177.3 |
C (mp-66) | <1 1 1> | <0 0 1> | 177.3 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 177.3 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 177.3 |
Mg (mp-153) | <1 0 1> | <0 1 0> | 187.6 |
TiO2 (mp-2657) | <1 1 0> | <1 0 0> | 116.0 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 295.6 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 295.6 |
PbS (mp-21276) | <1 0 0> | <1 0 1> | 141.6 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 177.3 |
BaTiO3 (mp-5986) | <0 0 1> | <0 0 1> | 236.5 |
BaTiO3 (mp-5986) | <1 0 1> | <1 0 0> | 116.0 |
InP (mp-20351) | <1 0 0> | <1 0 1> | 141.6 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 295.6 |
Ga2O3 (mp-886) | <1 0 0> | <1 0 -1> | 235.6 |
Au (mp-81) | <1 0 0> | <0 0 1> | 177.3 |
Au (mp-81) | <1 1 0> | <0 0 1> | 177.3 |
Ga2O3 (mp-886) | <0 1 0> | <1 0 1> | 141.6 |
Ga2O3 (mp-886) | <1 1 0> | <0 0 1> | 295.6 |
C (mp-48) | <0 0 1> | <0 0 1> | 295.6 |
C (mp-48) | <1 1 0> | <0 0 1> | 236.5 |
WSe2 (mp-1821) | <1 0 1> | <0 0 1> | 295.6 |
WSe2 (mp-1821) | <1 0 0> | <0 0 1> | 295.6 |
CaCO3 (mp-3953) | <0 0 1> | <0 0 1> | 177.3 |
CdWO4 (mp-19387) | <0 0 1> | <0 0 1> | 59.1 |
CdWO4 (mp-19387) | <1 0 1> | <0 0 1> | 177.3 |
TiO2 (mp-390) | <1 0 0> | <0 0 1> | 295.6 |
CdWO4 (mp-19387) | <0 1 0> | <0 0 1> | 295.6 |
ZnO (mp-2133) | <1 0 1> | <0 1 1> | 196.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Fe7O3F13 (mp-774072) | 0.5392 | 0.150 | 3 |
Mn6Zn3O16 (mp-774014) | 0.5132 | 0.355 | 3 |
Ti12Fe5O32 (mp-773987) | 0.5166 | 0.108 | 3 |
Ti6Co3O16 (mp-765900) | 0.5155 | 0.236 | 3 |
LiMo3O8 (mp-25584) | 0.5317 | 0.213 | 3 |
Zn3Cu10(TeO6)6 (mvc-15145) | 0.6856 | 0.063 | 4 |
KNi3As3O11 (mp-565287) | 0.6876 | 0.000 | 4 |
TaAl(WO4)2 (mvc-781) | 0.6033 | 0.297 | 4 |
MoO2 (mvc-6377) | 0.3808 | 0.295 | 2 |
FeO2 (mvc-13181) | 0.2794 | 0.757 | 2 |
FeO2 (mvc-12063) | 0.3523 | 0.842 | 2 |
CoO2 (mvc-5466) | 0.3109 | 0.285 | 2 |
NiO2 (mvc-6822) | 0.3290 | 0.483 | 2 |
Explore more synthesis descriptions for materials of composition MnO2.
Text computed by synthesisproject.org.
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Mn_pv O |
Final Energy/Atom-6.8981 eV |
Corrected Energy-380.4774 eV
-380.4774 eV = -331.1105 eV (uncorrected energy) - 26.8936 eV (MP Advanced Correction) - 22.4733 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)