Final Magnetic Moment1.808 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-3.083 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.225 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.15 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCaSiO3 + TiSi + Ti2O3 + SiO2 |
Band Gap0.193 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPbca [61] |
Hall-P 2ac 2ab |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 1 0> | <0 0 1> | 261.0 |
LaAlO3 (mp-2920) | <1 1 1> | <0 0 1> | 261.0 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 208.8 |
CeO2 (mp-20194) | <1 0 0> | <0 1 1> | 116.9 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 208.8 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 261.0 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 52.2 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 313.2 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 52.2 |
MoS2 (mp-1434) | <1 1 0> | <0 1 1> | 116.9 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 104.4 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 261.0 |
CdTe (mp-406) | <1 1 1> | <0 0 1> | 156.6 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 156.6 |
C (mp-66) | <1 1 0> | <0 0 1> | 261.0 |
GdScO3 (mp-5690) | <0 1 0> | <0 0 1> | 261.0 |
GdScO3 (mp-5690) | <1 1 1> | <0 0 1> | 208.8 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 52.2 |
Mg (mp-153) | <1 1 0> | <0 1 1> | 116.9 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 52.2 |
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 208.8 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 208.8 |
GaN (mp-804) | <1 1 0> | <0 1 1> | 116.9 |
SiO2 (mp-6930) | <1 1 0> | <0 1 1> | 233.9 |
KP(HO2)2 (mp-23959) | <0 0 1> | <0 1 1> | 233.9 |
KP(HO2)2 (mp-23959) | <0 1 0> | <0 1 1> | 233.9 |
LaF3 (mp-905) | <1 0 1> | <0 0 1> | 208.8 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 156.6 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 208.8 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 313.2 |
GaP (mp-2490) | <1 0 0> | <0 0 1> | 208.8 |
GaP (mp-2490) | <1 1 0> | <0 0 1> | 208.8 |
TbScO3 (mp-31119) | <0 0 1> | <0 0 1> | 156.6 |
TbScO3 (mp-31119) | <0 1 0> | <0 0 1> | 261.0 |
TbScO3 (mp-31119) | <0 1 1> | <0 0 1> | 52.2 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 208.8 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 313.2 |
TbScO3 (mp-31119) | <1 1 1> | <0 0 1> | 208.8 |
BN (mp-984) | <1 0 0> | <0 0 1> | 156.6 |
InSb (mp-20012) | <1 1 0> | <1 0 0> | 186.2 |
InSb (mp-20012) | <1 1 1> | <0 0 1> | 156.6 |
MoS2 (mp-1434) | <1 0 0> | <0 0 1> | 208.8 |
Al (mp-134) | <1 0 0> | <0 0 1> | 313.2 |
NdGaO3 (mp-3196) | <0 0 1> | <0 0 1> | 156.6 |
NdGaO3 (mp-3196) | <0 1 0> | <0 0 1> | 208.8 |
NdGaO3 (mp-3196) | <0 1 1> | <0 0 1> | 52.2 |
NdGaO3 (mp-3196) | <1 1 1> | <0 0 1> | 208.8 |
CdTe (mp-406) | <1 1 0> | <1 0 0> | 186.2 |
TiO2 (mp-2657) | <1 0 0> | <0 1 1> | 233.9 |
Ga2O3 (mp-886) | <1 0 0> | <0 0 1> | 313.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
FeSiO3 (mp-630331) | 0.3182 | 0.012 | 3 |
MgSiO3 (mp-557803) | 0.3719 | 0.011 | 3 |
MgSiO3 (mp-5834) | 0.3647 | 0.006 | 3 |
MgSiO3 (mp-1020124) | 0.3500 | 0.008 | 3 |
MgSiO3 (mp-1020123) | 0.3512 | 0.019 | 3 |
LiFe(SiO3)2 (mp-761416) | 0.2803 | 0.003 | 4 |
LiV(SiO3)2 (mp-766728) | 0.2856 | 0.003 | 4 |
MgMn(SiO3)2 (mvc-6876) | 0.2767 | 0.004 | 4 |
MnZn(SiO3)2 (mvc-6881) | 0.2695 | 0.040 | 4 |
CaV(SiO3)2 (mvc-6891) | 0.0993 | 0.073 | 4 |
VO2 (mvc-6918) | 0.7405 | 0.099 | 2 |
MoO2 (mvc-6944) | 0.6994 | 0.289 | 2 |
NaLi7Fe8(SiO3)16 (mp-775490) | 0.4131 | 0.003 | 5 |
Li3MnV(PO4)3 (mp-779876) | 0.4653 | 0.068 | 5 |
Li6ScFe5(SiO3)12 (mp-767482) | 0.4760 | 0.002 | 5 |
LiMnPO4F (mp-762774) | 0.4442 | 0.054 | 5 |
Li3MnV(PO4)3 (mp-780675) | 0.4771 | 0.034 | 5 |
Li4Mn3CuNi2(PO4)6 (mp-775323) | 0.5665 | 0.100 | 6 |
Li4CrCo2Ni3(PO4)6 (mp-776777) | 0.5680 | 0.094 | 6 |
Li4Mn3CrCo2(PO4)6 (mp-763479) | 0.5373 | 0.084 | 6 |
Li4MnCr2Fe3(PO4)6 (mp-779026) | 0.5519 | 0.099 | 6 |
Li4CrFe2Ni3(PO4)6 (mp-776753) | 0.5605 | 0.090 | 6 |
Ca2Al2FeSi4BHO16 (mp-540713) | 0.5705 | 0.002 | 7 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ca_sv Ti_pv Si O |
Final Energy/Atom-7.7001 eV |
Corrected Energy-649.7169 eV
-649.7169 eV = -616.0069 eV (uncorrected energy) - 33.7099 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)