Final Magnetic Moment4.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.875 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.087 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.89 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCa(CoO2)2 |
Band Gap0.387 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPc [7] |
HallP 2yc |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 150.5 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 31.5 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 210.7 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 157.5 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 283.6 |
CeO2 (mp-20194) | <1 1 1> | <0 1 1> | 217.9 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 150.5 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 301.0 |
GaAs (mp-2534) | <1 1 1> | <0 1 1> | 217.9 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 120.4 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 90.3 |
GaN (mp-804) | <1 0 0> | <0 1 1> | 130.7 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 150.5 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 297.9 |
GaN (mp-804) | <1 1 1> | <0 1 1> | 348.6 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 189.3 |
BN (mp-984) | <1 0 0> | <0 0 1> | 150.5 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 346.6 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 220.5 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 283.6 |
SiO2 (mp-6930) | <1 1 0> | <0 1 0> | 346.6 |
BN (mp-984) | <1 0 1> | <0 1 0> | 157.5 |
BN (mp-984) | <1 1 0> | <0 0 1> | 301.0 |
BN (mp-984) | <1 1 1> | <0 1 0> | 283.6 |
LiNbO3 (mp-3731) | <1 0 0> | <0 1 1> | 217.9 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 120.4 |
KCl (mp-23193) | <1 1 0> | <0 1 1> | 174.3 |
MoS2 (mp-1434) | <0 0 1> | <0 1 0> | 157.5 |
MoS2 (mp-1434) | <1 0 0> | <1 0 1> | 198.6 |
Al (mp-134) | <1 1 0> | <0 1 1> | 261.4 |
Al (mp-134) | <1 1 1> | <0 1 0> | 283.6 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 1> | 348.6 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 0> | 220.5 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 270.9 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 0> | 220.5 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 0> | 189.0 |
LiGaO2 (mp-5854) | <0 1 0> | <0 1 0> | 346.6 |
LiGaO2 (mp-5854) | <0 1 1> | <0 1 0> | 346.6 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 1> | 174.3 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 240.8 |
LiGaO2 (mp-5854) | <1 1 1> | <0 0 1> | 331.1 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 120.4 |
ZnSe (mp-1190) | <1 1 1> | <0 1 1> | 217.9 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 90.3 |
CdTe (mp-406) | <1 1 0> | <1 0 0> | 189.3 |
CdTe (mp-406) | <1 1 1> | <0 0 1> | 150.5 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 240.8 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 1> | 261.4 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 0> | 220.5 |
TeO2 (mp-2125) | <0 1 1> | <0 1 1> | 305.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
BaTl2O4 (mp-755315) | 0.3747 | 0.023 | 3 |
Ca(CuO2)2 (mvc-6054) | 0.3530 | 0.177 | 3 |
CaMn2O4 (mvc-6407) | 0.3797 | 0.046 | 3 |
Ca(CoO2)2 (mvc-6414) | 0.3654 | 0.089 | 3 |
Ca(NiO2)2 (mvc-6416) | 0.3886 | 0.041 | 3 |
CaTaNO2 (mp-556340) | 0.5516 | 0.011 | 4 |
HoZn(CoO3)2 (mvc-10230) | 0.5026 | 0.151 | 4 |
HoMg(CoO3)2 (mvc-10209) | 0.4625 | 0.140 | 4 |
Ca2YNiO5 (mvc-6231) | 0.5045 | 0.117 | 4 |
CaHo(CoO3)2 (mvc-10306) | 0.5526 | 0.084 | 4 |
Mn3O4 (mp-25696) | 0.5564 | 0.053 | 2 |
Fe3O4 (mp-18731) | 0.7452 | 0.106 | 2 |
Mn3O4 (mp-715570) | 0.4741 | 0.053 | 2 |
Ca5Gd3Ti5Mn3O24 (mp-744410) | 0.5234 | 0.013 | 5 |
Ca5Y3Ti5Mn3O24 (mp-743716) | 0.5323 | 0.020 | 5 |
Ca5Ho3Ti5Mn3O24 (mp-743699) | 0.5393 | 0.023 | 5 |
Ca5Dy3Ti5Mn3O24 (mp-743698) | 0.5314 | 0.020 | 5 |
CaSmMnSnO6 (mp-698702) | 0.5328 | 0.048 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCo: 3.32 eV |
PseudopotentialsVASP PAW: Ca_sv Co O |
Final Energy/Atom-6.0832 eV |
Corrected Energy-196.5581 eV
-196.5581 eV = -170.3295 eV (uncorrected energy) - 14.9920 eV (MP Advanced Correction) - 11.2366 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)