Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.300 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.157 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.38 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToW8O21 + Sb2WO6 + Y2WO6 + W |
Band Gap1.405 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP2/c [13] |
Hall-P 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 1> | 127.8 |
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 213.9 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 152.8 |
AlN (mp-661) | <0 0 1> | <0 1 1> | 127.8 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 280.6 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 122.2 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 213.9 |
AlN (mp-661) | <1 1 1> | <0 1 1> | 319.5 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 122.2 |
CeO2 (mp-20194) | <1 1 1> | <0 1 1> | 319.5 |
GaAs (mp-2534) | <1 0 0> | <1 0 -1> | 296.2 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 91.7 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 313.6 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 336.1 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 91.7 |
GaN (mp-804) | <1 0 0> | <1 0 1> | 236.7 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 244.4 |
GaN (mp-804) | <1 1 0> | <1 0 -1> | 59.2 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 62.7 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 213.9 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 275.0 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 91.7 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 313.6 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 30.6 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 91.7 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 336.1 |
ZnSe (mp-1190) | <1 0 0> | <1 0 -1> | 296.2 |
CdS (mp-672) | <0 0 1> | <1 1 1> | 290.5 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 244.4 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 313.6 |
Ag (mp-124) | <1 1 0> | <1 0 -1> | 296.2 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 1 1> | 290.5 |
GaSe (mp-1943) | <0 0 1> | <1 1 0> | 252.5 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 1 1> | 290.5 |
MoS2 (mp-1434) | <1 1 0> | <1 0 -1> | 118.5 |
MoS2 (mp-1434) | <1 1 1> | <1 0 1> | 236.7 |
Al (mp-134) | <1 1 1> | <0 0 1> | 275.0 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 -1> | 296.2 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 -1> | 177.7 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 91.7 |
TeO2 (mp-2125) | <0 1 0> | <0 0 1> | 213.9 |
TeO2 (mp-2125) | <1 0 0> | <0 0 1> | 213.9 |
LiTaO3 (mp-3666) | <0 0 1> | <0 1 0> | 280.6 |
LiTaO3 (mp-3666) | <1 0 0> | <1 0 -1> | 296.2 |
MgO (mp-1265) | <1 0 0> | <0 1 1> | 319.5 |
TiO2 (mp-2657) | <1 0 0> | <1 0 1> | 236.7 |
C (mp-66) | <1 0 0> | <1 1 -1> | 244.8 |
GdScO3 (mp-5690) | <0 1 1> | <0 0 1> | 213.9 |
GdScO3 (mp-5690) | <1 0 1> | <0 0 1> | 213.9 |
GdScO3 (mp-5690) | <1 1 0> | <1 1 0> | 252.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
EuTaO4 (mp-5957) | 0.4543 | 0.649 | 3 |
DyWO4 (mp-770600) | 0.4646 | 0.000 | 3 |
SrCaI4 (mp-752419) | 0.4867 | 0.076 | 3 |
ZrSiO4 (mp-1020588) | 0.4204 | 0.182 | 3 |
Zr5Ti7O24 (mp-761840) | 0.3188 | 0.030 | 3 |
EuTiClO3 (mp-555860) | 0.6340 | 0.000 | 4 |
ErAg(WO4)2 (mp-19655) | 0.6416 | 0.002 | 4 |
YNb2NO5 (mp-776359) | 0.6544 | 0.064 | 4 |
YBi(WO4)2 (mvc-679) | 0.3821 | 0.003 | 4 |
YSn(WO4)2 (mvc-705) | 0.2849 | 0.065 | 4 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesW: 6.2 eV |
PseudopotentialsVASP PAW: Y_sv Sb W_pv O |
Final Energy/Atom-7.4482 eV |
Corrected Energy-207.3978 eV
-207.3978 eV = -178.7571 eV (uncorrected energy) - 17.4040 eV (MP Advanced Correction) - 11.2366 eV (MP Anion Correction)
|