material

Ti(WO4)2

ID:

mvc-678

DOI:

10.17188/1322245


Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-2.387 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.152 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
5.49 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
WO3 + TiO2
Band Gap
2.713 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P1 [2]
Hall
-P 1
Point Group
1
Crystal System
triclinic

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
SiO2 (mp-6930) <1 0 0> <0 1 1> 0.000 193.5
Mg (mp-153) <1 0 0> <1 0 -1> 0.002 117.4
MgF2 (mp-1249) <0 0 1> <1 0 0> 0.003 66.2
InSb (mp-20012) <1 0 0> <1 0 0> 0.004 132.4
CdTe (mp-406) <1 0 0> <1 0 0> 0.005 132.4
GaN (mp-804) <1 1 0> <1 0 -1> 0.005 117.4
LiNbO3 (mp-3731) <1 0 0> <1 0 0> 0.006 297.9
GaN (mp-804) <1 0 0> <1 0 -1> 0.006 117.4
DyScO3 (mp-31120) <0 1 0> <1 1 1> 0.007 131.0
BaF2 (mp-1029) <1 0 0> <1 0 0> 0.008 198.6
ZrO2 (mp-2858) <0 0 1> <1 0 0> 0.009 165.5
C (mp-66) <1 1 0> <0 0 1> 0.009 126.8
ZnO (mp-2133) <0 0 1> <1 0 -1> 0.010 234.9
TbScO3 (mp-31119) <0 1 0> <1 1 1> 0.010 131.0
ZnSe (mp-1190) <1 1 0> <1 0 0> 0.014 231.7
LiAlO2 (mp-3427) <0 0 1> <1 0 0> 0.014 165.5
Te2W (mp-22693) <0 1 1> <1 0 1> 0.014 176.4
Ni (mp-23) <1 0 0> <1 0 0> 0.015 99.3
GaAs (mp-2534) <1 1 0> <1 0 0> 0.018 231.7
Si (mp-149) <1 0 0> <0 1 -1> 0.018 240.5
CeO2 (mp-20194) <1 0 0> <0 1 -1> 0.019 240.5
LiF (mp-1138) <1 1 0> <1 0 0> 0.021 165.5
CdS (mp-672) <1 0 0> <0 1 -1> 0.023 171.8
Te2W (mp-22693) <0 0 1> <1 -1 0> 0.025 197.8
CdWO4 (mp-19387) <1 0 0> <1 -1 0> 0.025 276.9
LiNbO3 (mp-3731) <1 0 1> <1 0 1> 0.025 308.8
Mg (mp-153) <1 1 0> <1 0 -1> 0.026 117.4
SiC (mp-8062) <1 1 0> <1 -1 1> 0.027 214.2
SiC (mp-7631) <0 0 1> <1 -1 0> 0.028 197.8
SiC (mp-11714) <0 0 1> <1 -1 0> 0.029 197.8
CdSe (mp-2691) <1 1 0> <1 -1 1> 0.030 214.2
ZnTe (mp-2176) <1 1 0> <1 -1 1> 0.031 214.2
Ge (mp-32) <1 1 0> <1 0 0> 0.032 231.7
GaP (mp-2490) <1 0 0> <0 1 -1> 0.032 240.5
YAlO3 (mp-3792) <1 0 0> <0 1 -1> 0.032 240.5
InAs (mp-20305) <1 1 0> <1 -1 1> 0.034 214.2
KTaO3 (mp-3614) <1 0 0> <1 1 0> 0.034 160.4
GaSb (mp-1156) <1 1 0> <1 -1 1> 0.035 214.2
LiAlO2 (mp-3427) <1 1 0> <1 0 0> 0.035 231.7
Al (mp-134) <1 0 0> <1 1 0> 0.037 160.4
GaTe (mp-542812) <1 0 -1> <0 1 0> 0.038 300.8
ZnO (mp-2133) <1 1 1> <0 0 1> 0.038 126.8
C (mp-48) <0 0 1> <0 1 0> 0.038 133.7
InP (mp-20351) <1 1 0> <1 -1 1> 0.038 299.9
MoSe2 (mp-1634) <1 0 1> <1 0 1> 0.040 264.7
Au (mp-81) <1 0 0> <1 0 0> 0.040 264.8
PbSe (mp-2201) <1 1 0> <1 -1 1> 0.044 214.2
TiO2 (mp-2657) <1 0 1> <1 0 0> 0.045 231.7
CaF2 (mp-2741) <1 0 0> <0 1 -1> 0.045 240.5
YAlO3 (mp-3792) <0 0 1> <1 0 0> 0.046 165.5
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
16 22 7 -5 0 8
22 142 29 -7 -3 43
7 29 97 -11 -3 9
-5 -7 -11 49 16 -5
0 -3 -3 16 13 -4
8 43 9 -5 -4 25
Compliance Tensor Sij (10-12Pa-1)
83.9 -7.8 -1.9 13.4 -24.9 -15.1
-7.8 16.1 -2.1 -0.3 -3.9 -25
-1.9 -2.1 11.2 2.1 -0.3 0.7
13.4 -0.3 2.1 36.8 -45.6 -4
-24.9 -3.9 -0.3 -45.6 139.1 27.2
-15.1 -25 0.7 -4 27.2 91.4
Shear Modulus GV
31 GPa
Bulk Modulus KV
41 GPa
Shear Modulus GR
12 GPa
Bulk Modulus KR
11 GPa
Shear Modulus GVRH
21 GPa
Bulk Modulus KVRH
26 GPa
Elastic Anisotropy
10.80
Poisson's Ratio
0.18

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
4.41 -0.19 -0.28
-0.19 5.10 -0.58
-0.28 -0.58 3.60
Dielectric Tensor εij (total)
17.23 0.48 -2.24
0.48 41.60 -11.39
-2.24 -11.39 8.65
Polycrystalline dielectric constant εpoly
(electronic contribution)
4.37
Polycrystalline dielectric constant εpoly
(total)
22.49
Refractive Index n
2.09
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Mo(WO4)2 (mvc-662) 0.2511 0.182 3
Sn(WO4)2 (mvc-668) 0.2570 0.154 3
V(WO4)2 (mvc-688) 0.1612 0.142 3
Cr(WO4)2 (mvc-708) 0.0839 0.165 3
Ni(WO4)2 (mvc-700) 0.3202 0.242 3
MgH2(SO4)2 (mp-690765) 0.6731 0.622 4
AsS6N5F6 (mp-558583) 0.6566 0.123 4
AsS7IF6 (mp-637112) 0.6472 0.000 4
SbSe3N2Cl7 (mp-570693) 0.6680 0.172 4
SnS16(Cl2O)2 (mp-614997) 0.6659 0.002 4
Ta2O5 (mp-676422) 0.7277 0.316 2
IO3 (mp-23315) 0.6590 0.051 2
Mn2F7 (mp-765941) 0.6427 0.033 2
W3O8 (mvc-671) 0.3112 0.186 2
MgCoH16(ClO2)4 (mp-743870) 0.7036 0.000 5
TiZnH12(OF)6 (mp-866807) 0.6439 0.020 5
FeH12Pt(ClO)6 (mp-542912) 0.7151 0.000 5
CaMg2H24(ClO2)6 (mp-696387) 0.7023 0.006 5
FeH12Pt(ClO)6 (mp-605175) 0.6411 0.000 5
AgAsS6N4(OF3)2 (mp-649756) 0.7390 0.142 6
AsSeS2N2ClF6 (mp-561321) 0.7117 0.065 6
Te2As2Se8S(OF6)2 (mp-557236) 0.7133 0.075 6
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA+U
Energy Cutoff
520 eV
# of K-points
None
U Values
W: 6.2 eV
Pseudopotentials
VASP PAW: Ti_pv W_pv O
Final Energy/Atom
-7.7576 eV
Corrected Energy
-99.7051 eV
Uncorrected energy = -85.3331 eV Composition-based energy adjustment (-0.687 eV/atom x 8.0 atoms) = -5.4960 eV Composition-based energy adjustment (-4.438 eV/atom x 2.0 atoms) = -8.8760 eV Corrected energy = -99.7051 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
Submitted by

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)