Final Magnetic Moment0.066 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-0.212 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.483 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.56 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNi3O4 + O2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCm [8] |
HallC 2y |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 287.3 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 218.2 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 185.0 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 57.5 |
ZnSe (mp-1190) | <1 0 0> | <1 0 1> | 132.1 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 109.1 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 229.9 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 185.0 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 287.3 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 -1> | 113.9 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 57.5 |
GaAs (mp-2534) | <1 0 0> | <1 0 1> | 132.1 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 185.0 |
LiF (mp-1138) | <1 0 0> | <1 0 1> | 132.1 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 114.9 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 57.5 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 114.9 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 264.1 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 172.4 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 172.4 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 172.4 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 57.5 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 114.9 |
BN (mp-984) | <0 0 1> | <0 0 1> | 114.9 |
Al (mp-134) | <1 0 0> | <0 0 1> | 287.3 |
Al (mp-134) | <1 1 0> | <1 0 -1> | 113.9 |
Al (mp-134) | <1 1 1> | <0 0 1> | 57.5 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 172.4 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 114.9 |
TeO2 (mp-2125) | <1 0 0> | <1 0 0> | 218.2 |
TeO2 (mp-2125) | <1 0 1> | <1 0 -1> | 227.8 |
TeO2 (mp-2125) | <0 0 1> | <1 0 -1> | 227.8 |
TiO2 (mp-2657) | <1 0 0> | <0 1 1> | 193.7 |
GdScO3 (mp-5690) | <0 0 1> | <1 0 0> | 218.2 |
C (mp-66) | <1 1 0> | <0 0 1> | 287.3 |
C (mp-66) | <1 1 1> | <0 0 1> | 172.4 |
GdScO3 (mp-5690) | <1 0 0> | <0 1 0> | 185.0 |
GdScO3 (mp-5690) | <1 0 1> | <0 0 1> | 57.5 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 114.9 |
TbScO3 (mp-31119) | <1 0 0> | <0 1 0> | 185.0 |
TbScO3 (mp-31119) | <1 0 1> | <0 0 1> | 57.5 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 172.4 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 172.4 |
TbScO3 (mp-31119) | <0 0 1> | <1 0 0> | 218.2 |
NdGaO3 (mp-3196) | <1 0 0> | <1 0 1> | 132.1 |
NdGaO3 (mp-3196) | <1 0 1> | <1 0 0> | 109.1 |
BaTiO3 (mp-5986) | <0 0 1> | <0 0 1> | 287.3 |
BaTiO3 (mp-5986) | <1 0 0> | <0 0 1> | 287.3 |
BaTiO3 (mp-5986) | <1 0 1> | <0 0 1> | 114.9 |
BaTiO3 (mp-5986) | <1 1 0> | <0 0 1> | 172.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
FeCo3O8 (mp-771554) | 0.5020 | 0.119 | 3 |
Li6Mn17O40 (mp-763817) | 0.5270 | 0.077 | 3 |
Al4(FeO4)3 (mvc-15002) | 0.5228 | 0.162 | 3 |
Mn6Zn3O16 (mp-774014) | 0.4820 | 0.355 | 3 |
LiMo3O8 (mp-25584) | 0.4943 | 0.215 | 3 |
Zn3Cu10(TeO6)6 (mvc-15145) | 0.7404 | 0.063 | 4 |
KNi3As3O11 (mp-565287) | 0.6922 | 0.000 | 4 |
TaAl(WO4)2 (mvc-781) | 0.7231 | 0.297 | 4 |
FeO2 (mvc-13181) | 0.2045 | 0.757 | 2 |
FeO2 (mvc-12063) | 0.3328 | 0.842 | 2 |
CoO2 (mvc-5466) | 0.1610 | 0.285 | 2 |
CrO2 (mvc-5295) | 0.4565 | 0.200 | 2 |
MnO2 (mvc-6353) | 0.3290 | 0.246 | 2 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesNi: 6.2 eV |
PseudopotentialsVASP PAW: Ni_pv O |
Final Energy/Atom-4.2479 eV |
Corrected Energy-260.9948 eV
-260.9948 eV = -203.8975 eV (uncorrected energy) - 34.6240 eV (MP Advanced Correction) - 22.4733 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)