Final Magnetic Moment3.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-3.067 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.084 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.20 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCa3V2(SiO4)3 + V2SiO4 + SiO2 + V3Si |
Band Gap2.180 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPbca [61] |
Hall-P 2ac 2ab |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 51.8 |
LaAlO3 (mp-2920) | <1 0 0> | <0 1 0> | 210.3 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 155.4 |
LaAlO3 (mp-2920) | <1 1 0> | <0 0 1> | 258.9 |
LaAlO3 (mp-2920) | <1 1 1> | <0 0 1> | 258.9 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 207.2 |
CeO2 (mp-20194) | <1 0 0> | <0 1 1> | 117.2 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 207.2 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 258.9 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 207.2 |
SiO2 (mp-6930) | <1 1 0> | <0 1 1> | 234.5 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 155.4 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 0> | 210.3 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 51.8 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 310.7 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 207.2 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 310.7 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 310.7 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 207.2 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 258.9 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 185.7 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 155.4 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 155.4 |
BN (mp-984) | <0 0 1> | <0 0 1> | 103.6 |
MoS2 (mp-1434) | <0 0 1> | <0 1 0> | 105.2 |
MoS2 (mp-1434) | <1 0 0> | <0 0 1> | 207.2 |
MoS2 (mp-1434) | <1 1 0> | <0 1 1> | 117.2 |
Al (mp-134) | <1 0 0> | <0 0 1> | 310.7 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 310.7 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 103.6 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 310.7 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 258.9 |
CdTe (mp-406) | <1 1 0> | <1 0 0> | 185.7 |
CdTe (mp-406) | <1 1 1> | <0 0 1> | 155.4 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 258.9 |
TiO2 (mp-2657) | <1 0 0> | <0 1 1> | 234.5 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 51.8 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 155.4 |
C (mp-66) | <1 1 0> | <0 0 1> | 258.9 |
GdScO3 (mp-5690) | <0 0 1> | <0 0 1> | 155.4 |
GdScO3 (mp-5690) | <0 1 0> | <0 0 1> | 258.9 |
GdScO3 (mp-5690) | <0 1 1> | <0 1 0> | 105.2 |
Mg (mp-153) | <0 0 1> | <0 1 0> | 105.2 |
Mg (mp-153) | <1 1 0> | <0 0 1> | 258.9 |
Mg (mp-153) | <1 1 1> | <0 0 1> | 207.2 |
KP(HO2)2 (mp-23959) | <0 0 1> | <0 1 1> | 234.5 |
KP(HO2)2 (mp-23959) | <0 1 0> | <0 1 1> | 234.5 |
LaF3 (mp-905) | <1 0 1> | <0 0 1> | 207.2 |
GaP (mp-2490) | <1 0 0> | <0 0 1> | 207.2 |
GaP (mp-2490) | <1 1 0> | <0 0 1> | 207.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
FeSiO3 (mp-630331) | 0.2721 | 0.014 | 3 |
MgSiO3 (mp-557803) | 0.3451 | 0.011 | 3 |
MgSiO3 (mp-1020125) | 0.3483 | 0.009 | 3 |
MgSiO3 (mp-1020124) | 0.3283 | 0.008 | 3 |
MgSiO3 (mp-1020123) | 0.3574 | 0.019 | 3 |
LiMn(SiO3)2 (mp-761776) | 0.2525 | 0.035 | 4 |
CaTi(SiO3)2 (mvc-6468) | 0.0993 | 0.222 | 4 |
MgMn(SiO3)2 (mvc-6876) | 0.2613 | 0.003 | 4 |
ZnCr(SiO3)2 (mvc-6877) | 0.2708 | 0.089 | 4 |
MnZn(SiO3)2 (mvc-6881) | 0.2485 | 0.042 | 4 |
MoO2 (mvc-6944) | 0.7121 | 0.281 | 2 |
NaLi7Fe8(SiO3)16 (mp-775490) | 0.4013 | 0.009 | 5 |
Li3MnV(PO4)3 (mp-779876) | 0.4824 | 0.219 | 5 |
Li6ScFe5(SiO3)12 (mp-767482) | 0.4834 | 0.005 | 5 |
Li3MnV(PO4)3 (mp-780675) | 0.4672 | 0.038 | 5 |
Li6MnV3(PO4)6 (mp-779387) | 0.4870 | 0.022 | 5 |
Li4Mn3CuNi2(PO4)6 (mp-775323) | 0.5542 | 0.083 | 6 |
Li4CrCo2Ni3(PO4)6 (mp-776777) | 0.5649 | 0.091 | 6 |
Li4Mn3CrCo2(PO4)6 (mp-763479) | 0.5473 | 0.081 | 6 |
Li4MnCr2Fe3(PO4)6 (mp-779026) | 0.5418 | 0.513 | 6 |
Li4CrFe2Ni3(PO4)6 (mp-776753) | 0.5627 | 0.399 | 6 |
Ca2Al2FeSi4BHO16 (mp-540713) | 0.5740 | 0.002 | 7 |
KNa2LiTi2Fe2(SiO3)8 (mp-542926) | 0.7300 | 0.000 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Ca_sv V_pv Si O |
Final Energy/Atom-7.6402 eV |
Corrected Energy-658.3811 eV
-658.3811 eV = -611.2152 eV (uncorrected energy) - 33.7099 eV (MP Anion Correction) - 13.4560 eV (MP Advanced Correction)
|