Final Magnetic Moment3.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.945 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.049 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.31 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCaSiO3 + Co2SiO4 + SiO2 |
Band Gap2.788 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPbca [61] |
Hall-P 2ac 2ab |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 0> | 102.6 |
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 205.3 |
CeO2 (mp-20194) | <1 1 0> | <0 1 0> | 205.3 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 210.4 |
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 210.4 |
AlN (mp-661) | <1 1 1> | <0 1 1> | 115.3 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 210.4 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 157.8 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 210.4 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 52.6 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 210.4 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 315.6 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 210.4 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 315.6 |
Te2Mo (mp-602) | <0 0 1> | <0 1 1> | 230.6 |
Al (mp-134) | <1 1 0> | <0 0 1> | 210.4 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 263.0 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 105.2 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 263.0 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 315.6 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 52.6 |
MoS2 (mp-1434) | <1 0 0> | <0 0 1> | 210.4 |
MoS2 (mp-1434) | <1 1 0> | <0 1 1> | 115.3 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 263.0 |
TiO2 (mp-2657) | <1 0 1> | <0 1 0> | 102.6 |
KP(HO2)2 (mp-23959) | <0 0 1> | <0 1 1> | 230.6 |
KP(HO2)2 (mp-23959) | <0 1 0> | <0 1 1> | 230.6 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 157.8 |
TiO2 (mp-2657) | <1 1 1> | <0 1 0> | 205.3 |
TbScO3 (mp-31119) | <0 0 1> | <0 0 1> | 157.8 |
TbScO3 (mp-31119) | <0 1 0> | <0 0 1> | 210.4 |
InSb (mp-20012) | <1 1 0> | <0 0 1> | 315.6 |
GdScO3 (mp-5690) | <0 0 1> | <0 0 1> | 157.8 |
GdScO3 (mp-5690) | <0 1 0> | <0 0 1> | 263.0 |
GdScO3 (mp-5690) | <0 1 1> | <0 0 1> | 52.6 |
GdScO3 (mp-5690) | <1 1 1> | <0 0 1> | 210.4 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 52.6 |
Mg (mp-153) | <1 1 0> | <0 1 1> | 115.3 |
Mg (mp-153) | <1 1 1> | <0 0 1> | 210.4 |
NdGaO3 (mp-3196) | <0 0 1> | <0 0 1> | 210.4 |
NdGaO3 (mp-3196) | <0 1 0> | <0 0 1> | 210.4 |
NdGaO3 (mp-3196) | <0 1 1> | <0 0 1> | 52.6 |
NdGaO3 (mp-3196) | <1 1 1> | <0 0 1> | 210.4 |
SiC (mp-11714) | <0 0 1> | <0 1 1> | 115.3 |
LaF3 (mp-905) | <1 0 1> | <0 0 1> | 210.4 |
GaP (mp-2490) | <1 0 0> | <0 0 1> | 210.4 |
GaP (mp-2490) | <1 1 0> | <0 0 1> | 210.4 |
TbScO3 (mp-31119) | <0 1 1> | <0 0 1> | 52.6 |
TbScO3 (mp-31119) | <1 1 1> | <0 0 1> | 210.4 |
Si (mp-149) | <1 0 0> | <0 1 0> | 205.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
FeSiO3 (mp-630331) | 0.3967 | 0.014 | 3 |
ZnSiO3 (mp-641917) | 0.3774 | 0.057 | 3 |
ZnSiO3 (mp-619034) | 0.3427 | 0.054 | 3 |
MnSiO3 (mp-19528) | 0.4192 | 0.007 | 3 |
MnSiO3 (mp-25041) | 0.4291 | 0.016 | 3 |
CaCu(SiO3)2 (mvc-6469) | 0.1324 | 0.088 | 4 |
CaMn(SiO3)2 (mvc-6888) | 0.1361 | 0.043 | 4 |
CaFe(SiO3)2 (mvc-6897) | 0.1143 | 0.041 | 4 |
CaCr(SiO3)2 (mvc-6906) | 0.3121 | 0.059 | 4 |
CaSi2NiO6 (mvc-6922) | 0.1767 | 0.061 | 4 |
NaLi7Fe8(SiO3)16 (mp-775490) | 0.4185 | 0.009 | 5 |
Li8Sc5Fe3(SiO3)16 (mp-775186) | 0.4513 | 0.004 | 5 |
Li5Sc2Fe3(SiO3)10 (mp-775172) | 0.4675 | 0.005 | 5 |
Li6ScFe5(SiO3)12 (mp-767482) | 0.4762 | 0.005 | 5 |
Li4ScFe3(SiO3)8 (mp-767448) | 0.4725 | 0.008 | 5 |
Li4Mn3CrCo2(PO4)6 (mp-763479) | 0.6066 | 0.081 | 6 |
Li4MnCr2Fe3(PO4)6 (mp-779026) | 0.6188 | 0.513 | 6 |
Li4Mn2VNi3(PO4)6 (mp-770417) | 0.5765 | 0.075 | 6 |
Li4TiMn3Cr2(PO4)6 (mp-778261) | 0.6084 | 0.081 | 6 |
Li4TiMn2Ni3(PO4)6 (mp-776756) | 0.6064 | 0.069 | 6 |
Ca2Al2FeSi4BHO16 (mp-540713) | 0.6239 | 0.002 | 7 |
KNa2LiTi2Fe2(SiO3)8 (mp-542926) | 0.6674 | 0.000 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCo: 3.32 eV |
PseudopotentialsVASP PAW: Ca_sv Co Si O |
Final Energy/Atom-7.3016 eV |
Corrected Energy-632.8284 eV
-632.8284 eV = -584.1264 eV (uncorrected energy) - 33.7099 eV (MP Anion Correction) - 14.9920 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)