Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingAFM |
Formation Energy / Atom-2.757 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.010 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.33 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCa2P2O7 + CaCo(PO3)4 + Co3(PO4)2 |
Band Gap2.773 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 0> | 178.7 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 1> | 307.5 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 178.7 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 190.0 |
AlN (mp-661) | <1 0 1> | <1 -1 1> | 122.9 |
AlN (mp-661) | <1 1 0> | <1 -1 -1> | 133.1 |
AlN (mp-661) | <1 1 1> | <1 -1 0> | 257.9 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 304.5 |
CeO2 (mp-20194) | <1 1 1> | <1 0 1> | 307.5 |
GaAs (mp-2534) | <1 1 0> | <0 1 -1> | 328.9 |
GaAs (mp-2534) | <1 1 1> | <0 1 0> | 178.7 |
BaF2 (mp-1029) | <1 0 0> | <0 1 1> | 311.2 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 265.9 |
GaN (mp-804) | <0 0 1> | <1 0 -1> | 179.1 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 152.0 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 134.0 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 265.9 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 312.7 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 330.6 |
SiO2 (mp-6930) | <1 0 1> | <1 1 1> | 176.4 |
SiO2 (mp-6930) | <1 1 0> | <1 1 0> | 152.2 |
SiO2 (mp-6930) | <1 1 1> | <0 1 0> | 268.0 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 330.6 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 190.0 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 -1> | 179.1 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 1> | 307.5 |
DyScO3 (mp-31120) | <1 0 1> | <1 -1 -1> | 332.7 |
DyScO3 (mp-31120) | <1 1 1> | <1 -1 0> | 206.3 |
InAs (mp-20305) | <1 0 0> | <1 0 -1> | 298.6 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 265.9 |
ZnSe (mp-1190) | <1 1 1> | <0 1 0> | 178.7 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 -1> | 274.1 |
KTaO3 (mp-3614) | <1 1 0> | <1 -1 1> | 184.4 |
KTaO3 (mp-3614) | <1 1 1> | <1 -1 -1> | 332.7 |
CdS (mp-672) | <0 0 1> | <1 -1 0> | 257.9 |
CdS (mp-672) | <1 0 0> | <1 1 0> | 228.3 |
CdS (mp-672) | <1 0 1> | <1 1 0> | 304.5 |
CdS (mp-672) | <1 1 0> | <1 -1 -1> | 199.6 |
LiF (mp-1138) | <1 1 0> | <1 -1 -1> | 266.2 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 190.0 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 236.2 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 190.0 |
Te2W (mp-22693) | <1 1 1> | <0 1 0> | 223.4 |
YVO4 (mp-19133) | <1 0 0> | <1 -1 0> | 309.5 |
YVO4 (mp-19133) | <1 0 1> | <1 -1 0> | 206.3 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 190.0 |
YVO4 (mp-19133) | <1 1 1> | <1 -1 1> | 245.9 |
TePb (mp-19717) | <1 0 0> | <1 0 1> | 307.5 |
TePb (mp-19717) | <1 1 0> | <0 1 0> | 312.7 |
Te2Mo (mp-602) | <0 0 1> | <1 -1 1> | 184.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Na2Ge2O5 (mp-772769) | 0.6153 | 0.022 | 3 |
Na2Si2O5 (mp-554383) | 0.5612 | 0.003 | 3 |
Na2Si2O5 (mp-556307) | 0.6403 | 0.001 | 3 |
MgTe2O7 (mvc-6996) | 0.6477 | 0.279 | 3 |
MnAs2O7 (mvc-8045) | 0.5947 | 0.131 | 3 |
CaTiP2O7 (mvc-6636) | 0.2399 | 0.206 | 4 |
CaMnP2O7 (mvc-6951) | 0.1783 | 0.013 | 4 |
CaVP2O7 (mvc-6957) | 0.1775 | 0.034 | 4 |
CaNiP2O7 (mvc-6949) | 0.0674 | 0.016 | 4 |
CaFeP2O7 (mvc-6954) | 0.1129 | 0.011 | 4 |
Na2Li2V3P2O13 (mp-853239) | 0.7355 | 0.061 | 5 |
KNaFe(Si2O5)2 (mp-19130) | 0.6433 | 0.000 | 5 |
KNaMn(Si2O5)2 (mp-647442) | 0.6470 | 0.000 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCo: 3.32 eV |
PseudopotentialsVASP PAW: Ca_sv Co P O |
Final Energy/Atom-7.1014 eV |
Corrected Energy-339.6217 eV
-339.6217 eV = -312.4616 eV (uncorrected energy) - 19.6641 eV (MP Anion Correction) - 7.4960 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)