Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.244 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.226 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.52 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToBiO2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP63/mmc [194] |
Hall-P 6c 2c |
Point Group6/mmm |
Crystal Systemhexagonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaTe (mp-542812) | <0 0 1> | <0 0 1> | 221.3 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 33.2 |
PbS (mp-21276) | <1 1 1> | <0 0 1> | 177.0 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 99.6 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 210.2 |
BN (mp-984) | <1 0 1> | <0 0 1> | 210.2 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 33.2 |
ZnTe (mp-2176) | <1 1 1> | <0 0 1> | 210.2 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 254.5 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 309.8 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 143.8 |
CaCO3 (mp-3953) | <0 0 1> | <0 0 1> | 210.2 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 276.6 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 143.8 |
C (mp-66) | <1 1 1> | <0 0 1> | 210.2 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 309.8 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 99.6 |
Fe3O4 (mp-19306) | <1 1 1> | <0 0 1> | 132.8 |
ZrO2 (mp-2858) | <0 0 1> | <0 0 1> | 232.4 |
ZrO2 (mp-2858) | <1 0 -1> | <0 0 1> | 265.6 |
NaCl (mp-22862) | <1 1 1> | <0 0 1> | 177.0 |
LiGaO2 (mp-5854) | <1 1 1> | <0 0 1> | 320.9 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 44.3 |
ZrO2 (mp-2858) | <0 1 1> | <0 0 1> | 166.0 |
CdSe (mp-2691) | <1 1 1> | <0 0 1> | 210.2 |
LiAlO2 (mp-3427) | <1 0 0> | <0 0 1> | 221.3 |
GaSb (mp-1156) | <1 1 1> | <0 0 1> | 210.2 |
SrTiO3 (mp-4651) | <1 0 1> | <0 0 1> | 154.9 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 132.8 |
BN (mp-984) | <0 0 1> | <0 0 1> | 99.6 |
YAlO3 (mp-3792) | <1 0 0> | <0 0 1> | 166.0 |
ZnO (mp-2133) | <0 0 1> | <0 0 1> | 143.8 |
PbSe (mp-2201) | <1 1 1> | <0 0 1> | 210.2 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 177.0 |
BaTiO3 (mp-5986) | <1 0 1> | <0 0 1> | 265.6 |
ZrO2 (mp-2858) | <1 1 1> | <0 0 1> | 265.6 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 77.5 |
CdWO4 (mp-19387) | <1 0 1> | <1 1 0> | 137.8 |
MgF2 (mp-1249) | <0 0 1> | <0 0 1> | 298.8 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 44.3 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 210.2 |
GaTe (mp-542812) | <1 0 -1> | <0 0 1> | 221.3 |
YAlO3 (mp-3792) | <0 1 1> | <0 0 1> | 99.6 |
Ge(Bi3O5)4 (mp-23352) | <1 1 1> | <0 0 1> | 177.0 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 143.8 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 77.5 |
SrTiO3 (mp-4651) | <1 0 0> | <0 0 1> | 298.8 |
GdScO3 (mp-5690) | <0 0 1> | <1 0 1> | 123.9 |
Te2W (mp-22693) | <1 0 0> | <1 1 1> | 279.1 |
YAlO3 (mp-3792) | <0 0 1> | <0 0 1> | 232.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
MnOF (mp-763196) | 0.6397 | 0.072 | 3 |
TlCoO3 (mp-770150) | 0.5966 | 0.054 | 3 |
CrSbO4 (mp-771809) | 0.6367 | 0.120 | 3 |
Sr2CaI6 (mp-756500) | 0.5725 | 0.062 | 3 |
LiRuN (mp-1029251) | 0.6332 | 0.000 | 3 |
LiV(OF)2 (mp-764229) | 0.6883 | 0.031 | 4 |
VO2 (mvc-11573) | 0.4687 | 0.267 | 2 |
SnO2 (mvc-6946) | 0.4043 | 0.162 | 2 |
WO2 (mvc-7369) | 0.3242 | 0.171 | 2 |
SbO2 (mvc-6936) | 0.0621 | 0.401 | 2 |
MoO2 (mvc-6948) | 0.3743 | 0.402 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Bi O |
Final Energy/Atom-5.3706 eV |
Corrected Energy-35.0330 eV
-35.0330 eV = -32.2239 eV (uncorrected energy) - 2.8092 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)