Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.319 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.380 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.50 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNiS2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI42d [122] |
HallI 4 2bw |
Point Group42m |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 1 1> | 203.6 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 266.4 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 77.3 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 231.8 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 222.0 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 231.8 |
CeO2 (mp-20194) | <1 1 1> | <1 0 0> | 310.8 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 128.8 |
BaF2 (mp-1029) | <1 0 0> | <1 0 1> | 205.3 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 222.0 |
BaF2 (mp-1029) | <1 1 1> | <1 0 0> | 133.2 |
GaN (mp-804) | <0 0 1> | <1 0 1> | 205.3 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 355.2 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 283.3 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 222.0 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 44.4 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 222.0 |
SiO2 (mp-6930) | <1 0 1> | <1 1 0> | 251.2 |
SiO2 (mp-6930) | <1 1 0> | <1 1 0> | 188.4 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 310.8 |
KCl (mp-23193) | <1 0 0> | <1 0 1> | 205.3 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 1> | 271.5 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 128.8 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 310.8 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 222.0 |
InAs (mp-20305) | <1 1 1> | <1 0 0> | 133.2 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 128.8 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 128.8 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 251.2 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 88.8 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 77.3 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 283.3 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 251.2 |
CdS (mp-672) | <1 1 1> | <1 1 0> | 314.0 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 128.8 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 355.2 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 88.8 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 180.3 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 266.4 |
Te2W (mp-22693) | <1 1 1> | <0 0 1> | 231.8 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 51.5 |
YVO4 (mp-19133) | <1 0 0> | <1 1 1> | 135.7 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 206.0 |
YVO4 (mp-19133) | <1 1 0> | <1 0 1> | 256.6 |
TePb (mp-19717) | <1 0 0> | <1 0 1> | 205.3 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 128.8 |
Te2Mo (mp-602) | <1 0 0> | <1 0 0> | 266.4 |
Te2Mo (mp-602) | <1 0 1> | <1 0 0> | 266.4 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 231.8 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 355.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
InPS4 (mp-20790) | 0.5793 | 0.000 | 3 |
K2B2S7 (mp-4351) | 0.6211 | 0.000 | 3 |
GaCuI4 (mp-29403) | 0.3189 | 0.000 | 3 |
AlCuCl4 (mp-28020) | 0.4177 | 0.000 | 3 |
GaCuCl4 (mp-29362) | 0.3839 | 0.000 | 3 |
HgI2 (mp-568742) | 0.2990 | 0.002 | 2 |
HgI2 (mp-583213) | 0.2487 | 0.000 | 2 |
SnS2 (mvc-7051) | 0.1301 | 0.065 | 2 |
WS2 (mvc-7053) | 0.1554 | 0.753 | 2 |
CeSe2 (mp-1080260) | 0.0794 | 0.507 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ni_pv S |
Final Energy/Atom-4.5608 eV |
Corrected Energy-30.0185 eV
-30.0185 eV = -27.3647 eV (uncorrected energy) - 2.6538 eV (MP Anion Correction)
|