Final Magnetic Moment0.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.007 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.047 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.62 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToBi2O3 + MgO |
Band Gap2.024 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 320.3 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 320.4 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 228.8 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 320.3 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 320.3 |
GaN (mp-804) | <1 0 0> | <1 1 0> | 134.7 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 178.0 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 178.0 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 228.8 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 320.4 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 183.0 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 284.8 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 356.0 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 106.8 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 284.8 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 142.4 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 106.8 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 320.4 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 320.3 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 320.4 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 106.8 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 178.0 |
Ag (mp-124) | <1 1 0> | <1 0 1> | 272.0 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 142.4 |
Ag (mp-124) | <1 1 1> | <1 0 0> | 249.2 |
BN (mp-984) | <0 0 1> | <1 0 0> | 320.4 |
BN (mp-984) | <1 0 0> | <1 0 0> | 178.0 |
BN (mp-984) | <1 1 0> | <0 0 1> | 320.3 |
BN (mp-984) | <1 0 1> | <1 0 0> | 320.4 |
LiNbO3 (mp-3731) | <1 0 1> | <1 0 0> | 320.4 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 284.8 |
MoS2 (mp-1434) | <0 0 1> | <1 0 1> | 272.0 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 320.4 |
Al (mp-134) | <1 0 0> | <1 0 0> | 213.6 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 178.0 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 178.0 |
TeO2 (mp-2125) | <0 1 1> | <0 0 1> | 228.8 |
TeO2 (mp-2125) | <1 0 1> | <0 0 1> | 228.8 |
CdTe (mp-406) | <1 0 0> | <1 0 1> | 136.0 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 320.3 |
MgO (mp-1265) | <1 1 0> | <1 0 1> | 204.0 |
MgO (mp-1265) | <1 1 1> | <1 0 0> | 249.2 |
TiO2 (mp-2657) | <1 0 1> | <1 0 0> | 249.2 |
MgO (mp-1265) | <1 0 0> | <1 0 1> | 272.0 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 106.8 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 249.2 |
TiO2 (mp-2657) | <1 1 0> | <1 0 0> | 284.8 |
C (mp-66) | <1 0 0> | <1 0 1> | 204.0 |
GdScO3 (mp-5690) | <0 1 1> | <0 0 1> | 274.5 |
Mg (mp-153) | <1 0 0> | <1 1 0> | 134.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Sr3La4O9 (mp-755969) | 0.5031 | 0.099 | 3 |
Mg(SbO2)2 (mvc-7317) | 0.5181 | 0.106 | 3 |
Ca(BiO2)2 (mvc-7276) | 0.4694 | 0.022 | 3 |
LiErO2 (mp-10970) | 0.5415 | 0.000 | 3 |
InSbS3 (mp-21365) | 0.4807 | 0.000 | 3 |
LiMnOF2 (mp-765334) | 0.6824 | 0.085 | 4 |
Li6MnAlO6 (mp-770706) | 0.6442 | 0.121 | 4 |
Li2Co2SiO6 (mp-763534) | 0.6521 | 0.141 | 4 |
Ca2SbWO6 (mvc-5995) | 0.6271 | 0.148 | 4 |
Ca2AgWO6 (mvc-5942) | 0.6327 | 0.086 | 4 |
Pb3O4 (mp-636813) | 0.5386 | 0.038 | 2 |
Cr3N4 (mp-1014365) | 0.7070 | 0.191 | 2 |
V23Se40 (mp-685047) | 0.6597 | 0.032 | 2 |
Ti3N4 (mp-1080192) | 0.6950 | 0.101 | 2 |
Tl4O3 (mp-27684) | 0.5981 | 0.000 | 2 |
NaLiV(OF)2 (mp-764851) | 0.5789 | 0.078 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Mg_pv Bi O |
Final Energy/Atom-5.7733 eV |
Corrected Energy-86.4444 eV
-86.4444 eV = -80.8261 eV (uncorrected energy) - 5.6183 eV (MP Anion Correction)
|