Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingAFM |
Formation Energy / Atom-1.955 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.144 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.12 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToV2CoO6 + V2Zn2O7 + CoO |
Band Gap1.303 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 1> | <0 1 0> | 229.7 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 306.3 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 278.3 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 278.3 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 306.3 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 0> | 306.3 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 92.8 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 185.5 |
Te2Mo (mp-602) | <0 0 1> | <1 0 -1> | 176.2 |
Te2W (mp-22693) | <0 0 1> | <1 0 -1> | 176.2 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 278.3 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 0> | 153.2 |
BN (mp-984) | <1 0 1> | <0 1 0> | 306.3 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 278.3 |
BN (mp-984) | <1 1 0> | <0 1 0> | 306.3 |
MoS2 (mp-1434) | <1 0 0> | <0 0 1> | 278.3 |
MoS2 (mp-1434) | <1 0 1> | <0 0 1> | 278.3 |
Al (mp-134) | <1 0 0> | <0 1 0> | 306.3 |
MoS2 (mp-1434) | <0 0 1> | <0 1 0> | 306.3 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 185.5 |
Al (mp-134) | <1 1 1> | <0 1 0> | 306.3 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 278.3 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 278.3 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 278.3 |
GdScO3 (mp-5690) | <1 1 1> | <0 0 1> | 278.3 |
Mg (mp-153) | <0 0 1> | <0 1 0> | 306.3 |
LaF3 (mp-905) | <1 0 1> | <0 0 1> | 278.3 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 278.3 |
TbScO3 (mp-31119) | <1 1 1> | <0 0 1> | 278.3 |
BaTiO3 (mp-5986) | <0 0 1> | <0 1 0> | 306.3 |
BaTiO3 (mp-5986) | <1 0 0> | <0 1 0> | 153.2 |
BaTiO3 (mp-5986) | <1 0 1> | <0 1 0> | 229.7 |
InSb (mp-20012) | <1 1 0> | <0 0 1> | 185.5 |
C (mp-48) | <1 1 1> | <0 1 0> | 306.3 |
Ga2O3 (mp-886) | <1 0 0> | <0 1 0> | 306.3 |
ZrO2 (mp-2858) | <0 0 1> | <0 1 0> | 306.3 |
ZrO2 (mp-2858) | <1 0 0> | <0 1 0> | 306.3 |
WS2 (mp-224) | <0 0 1> | <0 1 0> | 306.3 |
WS2 (mp-224) | <1 0 0> | <0 0 1> | 92.8 |
C (mp-48) | <0 0 1> | <0 0 1> | 278.3 |
C (mp-48) | <1 0 1> | <0 1 0> | 306.3 |
SiC (mp-8062) | <1 1 0> | <0 1 1> | 240.6 |
YAlO3 (mp-3792) | <0 0 1> | <0 1 0> | 306.3 |
TiO2 (mp-390) | <0 0 1> | <0 0 1> | 278.3 |
MgF2 (mp-1249) | <1 1 0> | <0 0 1> | 185.5 |
ZnO (mp-2133) | <0 0 1> | <0 1 0> | 306.3 |
ZnO (mp-2133) | <1 0 0> | <0 0 1> | 278.3 |
LiAlO2 (mp-3427) | <1 0 0> | <0 1 0> | 306.3 |
Al2O3 (mp-1143) | <1 0 0> | <0 0 1> | 185.5 |
GaTe (mp-542812) | <1 0 0> | <0 1 0> | 229.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cu4(PO4)3 (mp-673151) | 0.5468 | 0.039 | 3 |
Mg3(AsO4)2 (mp-770734) | 0.6336 | 0.065 | 3 |
Zn3(PO4)2 (mp-553958) | 0.6024 | 0.026 | 3 |
Cu3(AsO4)2 (mp-540858) | 0.6178 | 0.004 | 3 |
ZnCo3O7 (mvc-7796) | 0.6372 | 0.335 | 3 |
LiNi4(PO4)3 (mp-863906) | 0.4974 | 0.190 | 4 |
LiCu4(PO4)3 (mp-759742) | 0.5199 | 0.081 | 4 |
LiCr4(PO4)3 (mp-540459) | 0.4863 | 0.188 | 4 |
MgV2CoO7 (mvc-7648) | 0.3259 | 0.126 | 4 |
ZnCr2CoO7 (mvc-7782) | 0.3736 | 0.253 | 4 |
Na2Li2V3P2O13 (mp-853239) | 0.5944 | 0.061 | 5 |
Mg5Al4Fe(SiO4)6 (mp-743769) | 0.5702 | 0.280 | 5 |
Li2CuP3(HO5)2 (mp-849277) | 0.7068 | 0.083 | 5 |
NaMg3Si4O11F (mp-695597) | 0.6990 | 0.281 | 5 |
Li11Sc7Ti(PO4)12 (mp-695286) | 0.6544 | 0.637 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eVCo: 3.32 eV |
PseudopotentialsVASP PAW: V_pv Zn Co O |
Final Energy/Atom-6.5927 eV |
Corrected Energy-661.3911 eV
-661.3911 eV = -580.1588 eV (uncorrected energy) - 41.9040 eV (MP Advanced Correction) - 39.3282 eV (MP Anion Correction)
|