Final Magnetic Moment2.506 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.457 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.275 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.04 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToBaMoO3 + BaMoO4 + Y2O3 + Cu |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP4mm [99] |
HallP 4 2 |
Point Group4mm |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 32.5 |
GaAs (mp-2534) | <1 1 1> | <1 0 0> | 222.9 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 81.3 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 227.7 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 325.3 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 90.1 |
AlN (mp-661) | <1 1 0> | <1 1 1> | 239.4 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 254.8 |
GaN (mp-804) | <1 0 1> | <1 0 1> | 178.8 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 90.1 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 146.4 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 127.4 |
CeO2 (mp-20194) | <1 1 1> | <1 1 0> | 315.3 |
SiO2 (mp-6930) | <0 0 1> | <1 0 1> | 178.8 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 254.8 |
SiO2 (mp-6930) | <1 1 0> | <1 0 1> | 143.0 |
SiO2 (mp-6930) | <1 1 1> | <1 0 1> | 107.3 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 45.0 |
BaF2 (mp-1029) | <1 1 0> | <1 0 1> | 286.1 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 81.3 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 81.3 |
GaN (mp-804) | <1 0 0> | <1 1 0> | 180.2 |
GaN (mp-804) | <1 1 1> | <1 0 1> | 178.8 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 1> | 95.8 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 127.4 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 159.2 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 63.7 |
InAs (mp-20305) | <1 1 1> | <1 1 1> | 335.2 |
SiO2 (mp-6930) | <1 0 0> | <1 0 1> | 357.6 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 180.2 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 45.0 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 162.6 |
CdS (mp-672) | <0 0 1> | <1 0 1> | 250.3 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 254.8 |
CdS (mp-672) | <1 0 1> | <1 1 0> | 225.2 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 211.4 |
LiF (mp-1138) | <1 1 0> | <1 0 1> | 71.5 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 146.4 |
InAs (mp-20305) | <1 1 0> | <1 0 1> | 107.3 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 32.5 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 45.0 |
ZnSe (mp-1190) | <1 1 1> | <1 0 0> | 222.9 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 16.3 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 45.0 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 1> | 143.7 |
YVO4 (mp-19133) | <1 0 0> | <1 0 1> | 143.0 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 180.2 |
Te2Mo (mp-602) | <1 0 0> | <1 0 1> | 286.1 |
Te2Mo (mp-602) | <1 0 1> | <1 0 0> | 222.9 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 16.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
La2Fe2O5 (mp-1097052) | 0.6960 | 0.153 | 3 |
BaYFe2O5 (mp-542205) | 0.6495 | 0.108 | 4 |
BaDyFe2O5 (mp-24971) | 0.6464 | 0.028 | 4 |
BaYFeCuO5 (mp-505589) | 0.4303 | 0.007 | 5 |
BaYCuSbO5 (mvc-7194) | 0.4048 | 0.299 | 5 |
BaYCoCuO5 (mvc-7666) | 0.4023 | 0.035 | 5 |
BaYCrCuO5 (mvc-7667) | 0.3634 | 0.067 | 5 |
BaYCuWO5 (mvc-7676) | 0.4487 | 0.401 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMo: 4.38 eV |
PseudopotentialsVASP PAW: Ba_sv Y_sv Cu_pv Mo_pv O |
Final Energy/Atom-7.0161 eV |
Corrected Energy-70.1871 eV
-70.1871 eV = -63.1447 eV (uncorrected energy) - 3.5310 eV (MP Advanced Correction) - 3.5114 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)