Final Magnetic Moment0.015 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.406 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.165 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.69 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToBiO2 + ZnO |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP63mc [186] |
HallP 6c 2c |
Point Group6mm |
Crystal Systemhexagonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 1 0> | <1 0 0> | 130.5 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 199.0 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 278.6 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 261.0 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 159.2 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 326.2 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 278.6 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 261.0 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 278.6 |
DyScO3 (mp-31120) | <1 0 1> | <1 1 0> | 113.0 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 278.6 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 130.5 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 159.2 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 195.7 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 278.6 |
GaN (mp-804) | <1 0 1> | <1 1 0> | 113.0 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 199.0 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 195.7 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 261.0 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 195.7 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 195.7 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 159.2 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 261.0 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 119.4 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 278.6 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 278.6 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 199.0 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 0> | 113.0 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 199.0 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 119.4 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 119.4 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 358.2 |
GaSe (mp-1943) | <1 1 1> | <0 0 1> | 119.4 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 278.6 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 278.6 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 195.7 |
BN (mp-984) | <1 0 1> | <1 0 1> | 305.7 |
BN (mp-984) | <1 1 0> | <0 0 1> | 278.6 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 159.2 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 278.6 |
Al (mp-134) | <1 1 0> | <1 0 0> | 261.0 |
Al (mp-134) | <1 1 1> | <1 1 0> | 113.0 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 1> | 229.3 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 0> | 326.2 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 0> | 326.2 |
CdTe (mp-406) | <1 0 0> | <1 0 1> | 305.7 |
CdTe (mp-406) | <1 1 0> | <1 0 0> | 65.2 |
Al (mp-134) | <1 0 0> | <0 0 1> | 199.0 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 199.0 |
TiO2 (mp-2657) | <1 1 0> | <1 0 0> | 195.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Fe2Mo3O8 (mp-504974) | 0.2391 | 0.176 | 3 |
Mg2Sn3O8 (mvc-7646) | 0.3169 | 0.044 | 3 |
Mg2Bi3O8 (mvc-7627) | 0.1891 | 0.151 | 3 |
Mg2Sb3O8 (mvc-7639) | 0.2318 | 0.275 | 3 |
Zn2Sb3O8 (mvc-7691) | 0.2274 | 0.244 | 3 |
LiMn2O2F3 (mp-763878) | 0.5006 | 0.064 | 4 |
Li2Fe2OF6 (mp-777626) | 0.5234 | 0.041 | 4 |
LiYMo3O8 (mp-19431) | 0.5208 | 0.055 | 4 |
ScZnMo3O8 (mvc-16397) | 0.4288 | 0.072 | 4 |
LiV2O2F3 (mp-765244) | 0.5134 | 0.087 | 4 |
V3O5 (mp-714914) | 0.4893 | 0.004 | 2 |
V4O7 (mp-567080) | 0.5057 | 0.020 | 2 |
V3O5 (mp-714911) | 0.4770 | 0.003 | 2 |
V3O5 (mp-542441) | 0.4842 | 0.029 | 2 |
Ti3O5 (mp-556754) | 0.5113 | 0.013 | 2 |
Li4CrSb(WO6)2 (mp-764950) | 0.5460 | 0.037 | 5 |
Li4MnNb2WO12 (mp-771475) | 0.5730 | 0.047 | 5 |
Li4CrTe2WO12 (mp-775509) | 0.5712 | 0.109 | 5 |
Li4MnSb2WO12 (mp-763536) | 0.5645 | 0.069 | 5 |
Li4CrTe(WO6)2 (mp-777147) | 0.5407 | 0.075 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Zn Bi O |
Final Energy/Atom-5.1101 eV |
Corrected Energy-144.1003 eV
-144.1003 eV = -132.8637 eV (uncorrected energy) - 11.2366 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)