Final Magnetic Moment0.493 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-0.299 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.740 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.94 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToZn(NiO2)2 + CoO2 + O2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <1 0 0> | 146.0 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 295.3 |
GaAs (mp-2534) | <1 1 1> | <0 1 0> | 295.3 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 280.1 |
DyScO3 (mp-31120) | <1 0 1> | <1 1 0> | 163.6 |
ZnSe (mp-1190) | <1 1 1> | <0 1 0> | 295.3 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 221.5 |
Te2W (mp-22693) | <0 1 0> | <0 1 0> | 221.5 |
Te2W (mp-22693) | <0 1 1> | <0 1 1> | 119.0 |
Te2W (mp-22693) | <1 1 1> | <0 1 0> | 221.5 |
YVO4 (mp-19133) | <0 0 1> | <0 1 0> | 221.5 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 280.1 |
TePb (mp-19717) | <1 0 0> | <0 1 0> | 221.5 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 221.5 |
Te2Mo (mp-602) | <1 0 0> | <0 1 0> | 221.5 |
Te2Mo (mp-602) | <1 0 1> | <0 1 0> | 221.5 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 221.5 |
BN (mp-984) | <0 0 1> | <1 0 1> | 196.9 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 280.1 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 1> | 196.9 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 1> | 196.9 |
CdTe (mp-406) | <1 0 0> | <0 1 0> | 221.5 |
TeO2 (mp-2125) | <0 1 1> | <1 0 0> | 146.0 |
TiO2 (mp-2657) | <0 0 1> | <0 1 0> | 221.5 |
TiO2 (mp-2657) | <1 1 0> | <1 0 1> | 196.9 |
Ge3(BiO3)4 (mp-23560) | <1 0 0> | <0 1 0> | 221.5 |
C (mp-66) | <1 0 0> | <0 0 1> | 280.1 |
KP(HO2)2 (mp-23959) | <1 0 0> | <0 1 0> | 221.5 |
LaF3 (mp-905) | <0 0 1> | <0 1 0> | 221.5 |
LaF3 (mp-905) | <1 0 0> | <0 1 0> | 221.5 |
LaF3 (mp-905) | <1 0 1> | <0 0 1> | 280.1 |
TbScO3 (mp-31119) | <1 0 1> | <1 1 0> | 163.6 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 280.1 |
Ni (mp-23) | <1 0 0> | <0 1 0> | 73.8 |
InSb (mp-20012) | <1 0 0> | <0 1 0> | 221.5 |
BaTiO3 (mp-5986) | <0 0 1> | <0 1 1> | 238.1 |
SiC (mp-11714) | <1 0 1> | <0 1 0> | 295.3 |
SiC (mp-11714) | <1 1 0> | <0 0 1> | 280.1 |
Au (mp-81) | <1 0 0> | <0 1 0> | 221.5 |
WSe2 (mp-1821) | <1 0 0> | <1 0 1> | 196.9 |
ZrO2 (mp-2858) | <1 0 0> | <0 1 0> | 221.5 |
ZrO2 (mp-2858) | <0 0 1> | <0 1 0> | 221.5 |
Ge(Bi3O5)4 (mp-23352) | <1 0 0> | <0 1 0> | 221.5 |
YAlO3 (mp-3792) | <1 1 0> | <0 1 0> | 221.5 |
SiC (mp-8062) | <1 1 0> | <0 1 0> | 295.3 |
MgF2 (mp-1249) | <0 0 1> | <0 1 0> | 221.5 |
ZnO (mp-2133) | <1 0 0> | <0 0 1> | 280.1 |
Ge (mp-32) | <1 1 1> | <0 1 0> | 295.3 |
Al2O3 (mp-1143) | <1 0 0> | <0 0 1> | 186.7 |
Cu (mp-30) | <1 0 0> | <0 1 0> | 221.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Mg3(AsO4)2 (mp-675309) | 0.6541 | 0.655 | 3 |
Mn6O5F7 (mp-849517) | 0.7195 | 0.085 | 3 |
MgCo3O7 (mvc-7583) | 0.6754 | 0.342 | 3 |
Mg(SbO2)4 (mvc-10706) | 0.7236 | 0.194 | 3 |
ZnFe2CoO7 (mvc-7724) | 0.7055 | 0.255 | 4 |
MgFe2CoO7 (mvc-7571) | 0.5536 | 0.261 | 4 |
MgCoNi2O7 (mvc-7748) | 0.6069 | 0.705 | 4 |
ZnCoSn2O7 (mvc-8217) | 0.7076 | 0.281 | 4 |
CaCoSn2O7 (mvc-8260) | 0.6454 | 0.238 | 4 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCo: 3.32 eVNi: 6.2 eV |
PseudopotentialsVASP PAW: Zn Co Ni_pv O |
Final Energy/Atom-4.6030 eV |
Corrected Energy-462.8565 eV
-462.8565 eV = -405.0657 eV (uncorrected energy) - 49.6160 eV (MP Advanced Correction) - 8.1749 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)