Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.760 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.069 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.16 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToAs2O5 + WO3 + As2O3 |
Band Gap3.054 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 207.5 |
LaAlO3 (mp-2920) | <1 1 0> | <1 0 1> | 122.6 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 95.0 |
AlN (mp-661) | <1 1 1> | <0 1 1> | 201.6 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 220.1 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 285.1 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 276.7 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 285.1 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 146.7 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 207.5 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 293.4 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 285.1 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 276.7 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 220.1 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 207.5 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 69.2 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 190.1 |
TePb (mp-19717) | <1 1 0> | <1 0 1> | 122.6 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 138.3 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 276.7 |
BN (mp-984) | <0 0 1> | <0 1 0> | 220.1 |
LiNbO3 (mp-3731) | <1 0 1> | <1 1 0> | 240.1 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 0> | 293.4 |
MoS2 (mp-1434) | <0 0 1> | <0 1 1> | 201.6 |
Al (mp-134) | <1 1 1> | <1 0 0> | 285.1 |
CdTe (mp-406) | <1 1 0> | <1 0 1> | 122.6 |
Al (mp-134) | <1 0 0> | <0 1 0> | 146.7 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 0> | 285.1 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 138.3 |
SiC (mp-7631) | <0 0 1> | <1 0 0> | 190.1 |
SiC (mp-7631) | <1 1 1> | <1 1 0> | 240.1 |
LiTaO3 (mp-3666) | <1 0 1> | <1 1 0> | 240.1 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 276.7 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 207.5 |
TiO2 (mp-2657) | <1 0 0> | <0 1 0> | 220.1 |
TiO2 (mp-2657) | <1 1 0> | <0 1 0> | 293.4 |
C (mp-66) | <1 1 0> | <1 0 0> | 285.1 |
C (mp-66) | <1 0 0> | <0 0 1> | 207.5 |
GdScO3 (mp-5690) | <0 1 1> | <1 0 0> | 285.1 |
Mg (mp-153) | <0 0 1> | <0 1 1> | 201.6 |
Mg (mp-153) | <1 0 1> | <1 0 -1> | 112.2 |
LaF3 (mp-905) | <1 1 0> | <0 0 1> | 276.7 |
LaF3 (mp-905) | <1 0 0> | <0 0 1> | 207.5 |
TbScO3 (mp-31119) | <1 0 1> | <1 0 -1> | 112.2 |
InSb (mp-20012) | <1 1 0> | <1 0 1> | 122.6 |
BaTiO3 (mp-5986) | <1 0 0> | <0 1 0> | 220.1 |
BaTiO3 (mp-5986) | <1 1 1> | <1 0 0> | 285.1 |
BaTiO3 (mp-5986) | <0 0 1> | <0 1 0> | 146.7 |
NdGaO3 (mp-3196) | <0 1 1> | <0 0 1> | 207.5 |
SiC (mp-11714) | <1 0 0> | <1 0 0> | 95.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Mn(PO3)3 (mp-689966) | 0.5417 | 0.046 | 3 |
Fe(PO3)3 (mp-763780) | 0.5389 | 0.073 | 3 |
MgW2O7 (mvc-7373) | 0.4468 | 0.246 | 3 |
MgMo2O7 (mvc-7372) | 0.4911 | 0.113 | 3 |
MoAs2O7 (mvc-7986) | 0.4275 | 0.014 | 3 |
CaCu2(P2O7)2 (mvc-14848) | 0.6192 | 0.029 | 4 |
KAg(PO3)2 (mp-557874) | 0.5959 | 0.000 | 4 |
BaV(AsO4)2 (mp-566358) | 0.4773 | 0.012 | 4 |
Li2Sn(PO3)6 (mp-757479) | 0.6193 | 0.085 | 4 |
KV2PO8 (mp-566975) | 0.5940 | 0.000 | 4 |
Ca2Cu2Si3(HO3)4 (mp-696360) | 0.7375 | 0.178 | 5 |
LiVP3HO10 (mp-849441) | 0.6690 | 0.080 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesW: 6.2 eV |
PseudopotentialsVASP PAW: As W_pv O |
Final Energy/Atom-6.5250 eV |
Corrected Energy-298.0672 eV
-298.0672 eV = -260.9991 eV (uncorrected energy) - 19.6641 eV (MP Anion Correction) - 17.4040 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)