Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.409 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.052 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.45 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNb2SnO6 + ZnO |
Band Gap1.995 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 98.6 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 0> | 295.7 |
BN (mp-984) | <0 0 1> | <1 1 0> | 235.1 |
BN (mp-984) | <1 0 0> | <1 0 0> | 328.5 |
BN (mp-984) | <1 0 1> | <1 0 0> | 361.4 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 328.5 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 262.8 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 197.1 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 164.3 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 112.9 |
CeO2 (mp-20194) | <1 0 0> | <1 1 0> | 117.6 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 164.3 |
GaAs (mp-2534) | <1 1 1> | <1 1 1> | 173.4 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 230.0 |
MoS2 (mp-1434) | <1 1 0> | <0 1 0> | 112.9 |
MoS2 (mp-1434) | <1 1 1> | <1 0 0> | 230.0 |
Al (mp-134) | <1 1 0> | <1 0 0> | 164.3 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 361.4 |
GaN (mp-804) | <1 0 0> | <0 1 1> | 169.9 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 131.4 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 295.7 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 164.3 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 230.0 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 262.8 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 0> | 112.9 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 131.4 |
CdTe (mp-406) | <1 1 1> | <1 0 0> | 295.7 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 131.4 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 164.3 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 230.0 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 164.3 |
SiC (mp-7631) | <0 0 1> | <1 0 0> | 32.9 |
SiC (mp-7631) | <1 1 0> | <1 0 0> | 164.3 |
SiC (mp-7631) | <1 1 1> | <1 0 0> | 164.3 |
ZnSe (mp-1190) | <1 1 1> | <1 1 1> | 173.4 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 164.3 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 262.8 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 262.8 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 295.7 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 127.0 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 127.0 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 164.3 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 230.0 |
TiO2 (mp-2657) | <1 0 1> | <1 0 0> | 98.6 |
TiO2 (mp-2657) | <1 1 0> | <1 0 0> | 131.4 |
TiO2 (mp-2657) | <1 1 1> | <1 0 0> | 197.1 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 361.4 |
C (mp-66) | <1 0 0> | <1 0 0> | 164.3 |
C (mp-66) | <1 1 0> | <1 0 0> | 164.3 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 295.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
VZnO2 (mvc-12242) | 0.6102 | 0.297 | 3 |
CoAgO3 (mp-761547) | 0.6128 | 0.481 | 3 |
CaBi2O5 (mp-772874) | 0.5832 | 0.034 | 3 |
CaBi2O5 (mvc-8883) | 0.5844 | 0.078 | 3 |
VIn2O5 (mp-25723) | 0.5741 | 0.031 | 3 |
Nb2Zn2BiO8 (mvc-2) | 0.2776 | 0.098 | 4 |
Mg2Ta2SnO8 (mvc-2377) | 0.3270 | 0.061 | 4 |
Ta2Zn2SnO8 (mvc-2362) | 0.1819 | 0.058 | 4 |
Mg2Nb2SnO8 (mvc-3358) | 0.3730 | 0.054 | 4 |
Mg2Nb2BiO8 (mvc-13297) | 0.3470 | 0.120 | 4 |
Li4MnV(WO6)2 (mp-761440) | 0.5399 | 0.049 | 5 |
Li4MnNb(WO6)2 (mp-771868) | 0.6121 | 0.027 | 5 |
Li4VTe(WO6)2 (mp-778316) | 0.5828 | 0.056 | 5 |
Li4CrFe(WO6)2 (mp-770069) | 0.6134 | 0.550 | 5 |
Li4MnV2WO12 (mp-773239) | 0.5413 | 0.089 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Nb_pv Zn Sn_d O |
Final Energy/Atom-7.0783 eV |
Corrected Energy-195.2725 eV
-195.2725 eV = -184.0358 eV (uncorrected energy) - 11.2366 eV (MP Anion Correction)
|