Final Magnetic Moment3.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-1.830 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.087 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.91 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCa2Co3O8 |
Band Gap0.043 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP63mc [186] |
HallP 6c 2c |
Point Group6mm |
Crystal Systemhexagonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 207.0 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 325.2 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 121.8 |
AlN (mp-661) | <1 1 0> | <1 1 1> | 109.6 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 207.0 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 236.5 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 236.5 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 207.0 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 118.3 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 304.6 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 243.7 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 270.8 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 88.7 |
SiO2 (mp-6930) | <1 0 0> | <1 1 1> | 109.6 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 207.0 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 295.7 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 182.7 |
DyScO3 (mp-31120) | <1 1 1> | <1 1 1> | 219.1 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 207.0 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 236.5 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 236.5 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 147.8 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 118.3 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 29.6 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 207.0 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 354.8 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 304.6 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 147.8 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 118.3 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 29.6 |
YVO4 (mp-19133) | <0 0 1> | <1 1 0> | 105.5 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 207.0 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 266.1 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 88.7 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 118.3 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 29.6 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 118.3 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 88.7 |
BN (mp-984) | <0 0 1> | <0 0 1> | 88.7 |
BN (mp-984) | <1 0 1> | <1 1 1> | 219.1 |
BN (mp-984) | <1 1 0> | <1 0 0> | 243.7 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 207.0 |
LiNbO3 (mp-3731) | <1 0 1> | <1 0 0> | 304.6 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 207.0 |
Al (mp-134) | <1 0 0> | <0 0 1> | 147.8 |
Al (mp-134) | <1 1 0> | <0 0 1> | 118.3 |
Al (mp-134) | <1 1 1> | <0 0 1> | 29.6 |
LiGaO2 (mp-5854) | <0 0 1> | <1 1 1> | 109.6 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 266.1 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 354.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ca2Ti3O8 (mvc-7709) | 0.2868 | 0.094 | 3 |
Ca2Mn3O8 (mvc-8030) | 0.3700 | 0.105 | 3 |
Ca2V3O8 (mvc-8051) | 0.2761 | 0.097 | 3 |
Ca2Cr3O8 (mvc-8059) | 0.2298 | 0.114 | 3 |
Ca2Fe3O8 (mvc-8063) | 0.1901 | 0.130 | 3 |
MgCo(GeO3)2 (mvc-8335) | 0.5588 | 0.005 | 4 |
MgV(GeO3)2 (mvc-8338) | 0.5918 | 0.033 | 4 |
MgNi(GeO3)2 (mvc-8356) | 0.5617 | 0.008 | 4 |
MgFe(GeO3)2 (mvc-8596) | 0.5876 | 0.007 | 4 |
ZnCr(GeO3)2 (mvc-8435) | 0.5959 | 0.088 | 4 |
Fe21O32 (mp-698578) | 0.6166 | 0.195 | 2 |
Mn2O3 (mp-779818) | 0.6184 | 0.079 | 2 |
Fe43O64 (mp-705779) | 0.6335 | 0.116 | 2 |
Fe2O3 (mp-705773) | 0.6482 | 0.225 | 2 |
Fe5O8 (mp-543082) | 0.6038 | 0.163 | 2 |
Li4Nb3Fe3(SbO8)2 (mp-868012) | 0.7148 | 0.067 | 5 |
Li4Mn3Nb3(SbO8)2 (mp-773620) | 0.7003 | 0.086 | 5 |
Li4Nb3Cu3(TeO8)2 (mp-774886) | 0.7302 | 0.096 | 5 |
MgTi2Be3(SiO4)3 (mvc-10530) | 0.7294 | 0.201 | 5 |
Ti2Be3Zn(SiO4)3 (mvc-10526) | 0.7004 | 0.233 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCo: 3.32 eV |
PseudopotentialsVASP PAW: Ca_sv Co O |
Final Energy/Atom-5.9591 eV |
Corrected Energy-177.4172 eV
-177.4172 eV = -154.9366 eV (uncorrected energy) - 11.2440 eV (MP Advanced Correction) - 11.2366 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)