Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.520 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.131 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.51 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTiO2 + MgGeO3 + Ge + GeO2 |
Band Gap1.442 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 274.9 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 267.0 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 161.0 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 222.5 |
GaAs (mp-2534) | <1 0 0> | <0 1 0> | 268.3 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 274.9 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 278.8 |
GaN (mp-804) | <0 0 1> | <1 1 0> | 278.8 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 133.5 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 268.3 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 311.4 |
GaN (mp-804) | <1 1 1> | <1 1 0> | 278.8 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 44.5 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 222.5 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 222.5 |
SiO2 (mp-6930) | <1 1 0> | <1 0 -1> | 93.3 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 311.4 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 222.5 |
InAs (mp-20305) | <1 1 0> | <1 0 1> | 109.7 |
InAs (mp-20305) | <1 1 1> | <1 0 0> | 133.5 |
ZnSe (mp-1190) | <1 0 0> | <0 1 0> | 268.3 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 0> | 322.0 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 311.4 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 133.5 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 268.3 |
LiF (mp-1138) | <1 1 1> | <0 1 0> | 322.0 |
Te2W (mp-22693) | <0 1 0> | <1 1 0> | 209.1 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 267.0 |
YVO4 (mp-19133) | <1 1 0> | <0 1 0> | 322.0 |
Te2Mo (mp-602) | <1 0 0> | <1 1 0> | 209.1 |
YVO4 (mp-19133) | <1 0 0> | <0 1 0> | 322.0 |
Ag (mp-124) | <1 1 0> | <1 0 1> | 219.4 |
Ag (mp-124) | <1 1 1> | <0 1 0> | 322.0 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 214.7 |
BN (mp-984) | <0 0 1> | <1 0 1> | 109.7 |
BN (mp-984) | <1 0 0> | <0 1 1> | 212.4 |
BN (mp-984) | <1 1 0> | <1 0 0> | 133.5 |
BN (mp-984) | <1 1 1> | <1 0 0> | 133.5 |
LiNbO3 (mp-3731) | <1 0 0> | <1 0 0> | 222.5 |
LiNbO3 (mp-3731) | <1 0 1> | <1 0 0> | 311.4 |
BN (mp-984) | <1 0 1> | <1 0 0> | 222.5 |
Al (mp-134) | <1 1 1> | <0 1 0> | 322.0 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 311.4 |
MoS2 (mp-1434) | <0 0 1> | <1 0 -1> | 280.0 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 44.5 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 0> | 222.5 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 133.5 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 0> | 268.3 |
LiGaO2 (mp-5854) | <1 0 1> | <0 1 0> | 268.3 |
SiC (mp-7631) | <0 0 1> | <0 1 0> | 268.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li2VF4 (mp-853172) | 0.4396 | 0.193 | 3 |
TiCrO3 (mp-769925) | 0.5680 | 0.119 | 3 |
Li3VF6 (mp-763439) | 0.5580 | 0.037 | 3 |
CaMn4O8 (mp-1003320) | 0.5570 | 0.059 | 3 |
Na4ZnSe3 (mp-1094105) | 0.5259 | 0.054 | 3 |
TiZn(GeO3)2 (mvc-8118) | 0.3891 | 0.130 | 4 |
Mg2Nb2CoO8 (mvc-3391) | 0.5542 | 0.018 | 4 |
Mg2Nb2CrO8 (mvc-415) | 0.5594 | 0.513 | 4 |
Mg2MnNb2O8 (mvc-402) | 0.5678 | 0.220 | 4 |
Mg2Nb2NiO8 (mvc-418) | 0.5638 | 0.071 | 4 |
Fe2O3 (mp-628327) | 0.7443 | 0.749 | 2 |
Pb3O4 (mp-21452) | 0.7146 | 0.000 | 2 |
V2O3 (mp-776688) | 0.6583 | 0.087 | 2 |
V5O9 (mp-704305) | 0.7449 | 0.008 | 2 |
Li4FeTe(WO6)2 (mp-771716) | 0.6987 | 0.163 | 5 |
Li4MnSb(WO6)2 (mp-779994) | 0.7023 | 0.041 | 5 |
Li4CrTe(WO6)2 (mp-777147) | 0.7327 | 0.075 | 5 |
Li4VCr(WO6)2 (mp-761696) | 0.6214 | 0.050 | 5 |
Li4VFe(WO6)2 (mp-761519) | 0.6393 | 0.070 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Mg_pv Ti_pv Ge_d O |
Final Energy/Atom-6.9419 eV |
Corrected Energy-147.2659 eV
-147.2659 eV = -138.8384 eV (uncorrected energy) - 8.4275 eV (MP Anion Correction)
|