Final Magnetic Moment20.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.947 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.118 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.44 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCaTa2O6 + Fe2O3 |
Band Gap2.740 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 1 0> | 220.6 |
GaN (mp-804) | <0 0 1> | <1 1 -1> | 240.8 |
GaN (mp-804) | <1 0 0> | <0 1 -1> | 291.0 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 293.8 |
SiO2 (mp-6930) | <1 0 1> | <1 -1 0> | 180.0 |
KCl (mp-23193) | <1 1 0> | <0 1 0> | 294.2 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 293.8 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 260.8 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 293.8 |
YVO4 (mp-19133) | <1 0 1> | <1 -1 0> | 270.0 |
TePb (mp-19717) | <1 1 0> | <0 1 0> | 294.2 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 294.2 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 293.8 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 293.8 |
LaAlO3 (mp-2920) | <1 0 1> | <1 -1 -1> | 218.2 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 0> | 294.2 |
BN (mp-984) | <0 0 1> | <0 0 1> | 235.1 |
BN (mp-984) | <1 0 0> | <1 0 -1> | 176.6 |
BN (mp-984) | <1 1 0> | <1 0 -1> | 264.9 |
BN (mp-984) | <1 1 1> | <1 0 1> | 238.6 |
GaAs (mp-2534) | <1 1 1> | <0 1 0> | 220.6 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 220.6 |
LiNbO3 (mp-3731) | <1 0 0> | <0 0 1> | 293.8 |
ZnSe (mp-1190) | <1 1 1> | <0 1 0> | 220.6 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 260.8 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 260.8 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 293.8 |
MoS2 (mp-1434) | <0 0 1> | <1 0 1> | 238.6 |
LiGaO2 (mp-5854) | <1 1 1> | <1 0 -1> | 176.6 |
SiC (mp-7631) | <0 0 1> | <1 1 -1> | 240.8 |
MgO (mp-1265) | <1 1 1> | <0 1 -1> | 218.3 |
LiTaO3 (mp-3666) | <1 0 0> | <0 0 1> | 293.8 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 235.1 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 176.3 |
MgO (mp-1265) | <1 1 0> | <0 1 -1> | 291.0 |
TiO2 (mp-2657) | <1 1 0> | <0 1 -1> | 291.0 |
C (mp-66) | <1 0 0> | <0 1 0> | 294.2 |
C (mp-66) | <1 1 0> | <0 0 1> | 293.8 |
Mg (mp-153) | <1 0 0> | <1 -1 -1> | 218.2 |
GdScO3 (mp-5690) | <0 1 0> | <0 0 1> | 293.8 |
LaF3 (mp-905) | <1 1 1> | <0 1 -1> | 218.3 |
GaP (mp-2490) | <1 1 1> | <0 1 0> | 220.6 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 293.8 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 293.8 |
TbScO3 (mp-31119) | <0 1 0> | <0 0 1> | 293.8 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 235.1 |
Ni (mp-23) | <1 1 0> | <0 1 -1> | 291.0 |
PbSe (mp-2201) | <1 1 0> | <0 1 0> | 220.6 |
BaTiO3 (mp-5986) | <1 0 0> | <1 -1 -1> | 218.2 |
BaTiO3 (mp-5986) | <1 1 0> | <0 0 1> | 293.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cr5(PO4)4 (mp-540446) | 0.6435 | 0.007 | 3 |
Mg2V2O7 (mp-32500) | 0.5982 | 0.000 | 3 |
Cr5(PO4)4 (mp-775246) | 0.6491 | 0.007 | 3 |
V3ZnO8 (mp-649966) | 0.6580 | 0.007 | 3 |
V3CoO8 (mp-861528) | 0.6018 | 0.003 | 3 |
Li2Mn2(PO4)3 (mp-774345) | 0.6021 | 0.024 | 4 |
Li2Mn2(PO4)3 (mp-762743) | 0.6098 | 0.018 | 4 |
Ca3V6(FeO6)4 (mvc-7981) | 0.5996 | 0.016 | 4 |
Ca3Fe4(WO4)6 (mvc-8255) | 0.5845 | 0.102 | 4 |
Ca3Fe4(MoO4)6 (mvc-8288) | 0.5974 | 0.081 | 4 |
LiVP2HO8 (mp-780110) | 0.6544 | 0.047 | 5 |
NaMg3Al(MoO4)5 (mp-561496) | 0.6092 | 0.007 | 5 |
Li3V2P4(HO8)2 (mp-781078) | 0.6354 | 0.064 | 5 |
Li3V2P4(HO8)2 (mp-781013) | 0.6585 | 0.067 | 5 |
Li3V2P4(HO8)2 (mp-776714) | 0.6379 | 0.000 | 5 |
LiVFeP2(O4F)2 (mp-777635) | 0.6495 | 0.028 | 6 |
LiVCrP2(O4F)2 (mp-767464) | 0.6474 | 0.011 | 6 |
LiVCrP2(O4F)2 (mp-868574) | 0.6558 | 0.006 | 6 |
Na3Mg4CrSi8(O11F)2 (mp-743787) | 0.5989 | 0.709 | 6 |
LiVCrP2(O4F)2 (mp-765118) | 0.6545 | 0.007 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Ca_sv Ta_pv Fe_pv O |
Final Energy/Atom-8.4063 eV |
Corrected Energy-338.8189 eV
-338.8189 eV = -311.0320 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction) - 10.9320 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)