Final Magnetic Moment9.004 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-1.505 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.081 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.17 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCu2O3 + Mg(CuO2)2 + Fe2O3 + O2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinIm3 [204] |
Hall-I 2 2 3 |
Point Groupm3 |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 1> | <1 1 0> | 233.5 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 275.2 |
GaN (mp-804) | <0 0 1> | <1 1 0> | 311.3 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 233.5 |
SiO2 (mp-6930) | <1 0 1> | <1 1 0> | 311.3 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 155.7 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 155.7 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 275.2 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 275.2 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 275.2 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 155.7 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 220.1 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 233.5 |
BaF2 (mp-1029) | <1 1 1> | <1 1 1> | 285.9 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 165.1 |
SiO2 (mp-6930) | <0 0 1> | <1 1 1> | 285.9 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 311.3 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 233.5 |
KCl (mp-23193) | <1 1 1> | <1 1 1> | 285.9 |
YVO4 (mp-19133) | <1 0 0> | <1 1 0> | 233.5 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 220.1 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 220.1 |
Te2Mo (mp-602) | <1 0 1> | <1 1 1> | 285.9 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 220.1 |
GaSe (mp-1943) | <1 1 0> | <1 1 0> | 233.5 |
InAs (mp-20305) | <1 1 1> | <1 0 0> | 330.2 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 275.2 |
Te2W (mp-22693) | <1 1 0> | <1 1 0> | 233.5 |
MoS2 (mp-1434) | <0 0 1> | <1 1 0> | 311.3 |
Al (mp-134) | <1 0 0> | <1 0 0> | 275.2 |
LiGaO2 (mp-5854) | <0 0 1> | <1 1 1> | 285.9 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 275.2 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 55.0 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 330.2 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 233.5 |
TePb (mp-19717) | <1 1 1> | <1 1 1> | 285.9 |
Ag (mp-124) | <1 1 1> | <1 0 0> | 275.2 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 275.2 |
SiC (mp-7631) | <0 0 1> | <1 0 0> | 165.1 |
SiC (mp-7631) | <1 0 0> | <1 0 0> | 330.2 |
GaSe (mp-1943) | <1 0 1> | <1 0 0> | 275.2 |
LiNbO3 (mp-3731) | <0 0 1> | <1 1 1> | 95.3 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 275.2 |
LiTaO3 (mp-3666) | <0 0 1> | <1 1 1> | 95.3 |
LiTaO3 (mp-3666) | <1 0 0> | <1 1 1> | 285.9 |
LiGaO2 (mp-5854) | <1 1 0> | <1 1 0> | 233.5 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 0> | 275.2 |
MgO (mp-1265) | <1 1 0> | <1 1 0> | 77.8 |
MgO (mp-1265) | <1 1 1> | <1 1 1> | 95.3 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 110.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LaMn7O12 (mp-567029) | 0.1692 | 0.065 | 3 |
CaMn7O12 (mp-541644) | 0.1674 | 0.020 | 3 |
PrMn7O12 (mp-19354) | 0.2322 | 0.022 | 3 |
YCu7O12 (mvc-1832) | 0.1922 | 0.000 | 3 |
PrMn7O12 (mp-567134) | 0.1921 | 0.022 | 3 |
CaCu3(SnO3)4 (mp-18190) | 0.0806 | 0.064 | 4 |
ZnCu3(SnO3)4 (mvc-7867) | 0.0710 | 0.161 | 4 |
ZnCr4(CuO4)3 (mvc-8313) | 0.0438 | 0.083 | 4 |
Mn4Zn(CuO4)3 (mvc-8312) | 0.0681 | 0.095 | 4 |
CaCu3(SnO3)4 (mvc-16303) | 0.0806 | 0.064 | 4 |
CaCr2Cu3(SbO6)2 (mp-510534) | 0.2345 | 0.060 | 5 |
CaNb2Ga2(CuO4)3 (mp-686705) | 0.2335 | 0.111 | 5 |
CaTa2Ga2(CuO4)3 (mp-694913) | 0.2340 | 0.000 | 5 |
CaGa2Cu3(SbO6)2 (mp-41331) | 0.2253 | 0.080 | 5 |
CaGa2Cu3(RuO6)2 (mp-720504) | 0.1995 | 0.029 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Mg_pv Fe_pv Cu_pv O |
Final Energy/Atom-5.8947 eV |
Corrected Energy-137.2542 eV
-137.2542 eV = -117.8947 eV (uncorrected energy) - 10.9320 eV (MP Advanced Correction) - 8.4275 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)