Final Magnetic Moment2.082 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.300 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.139 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.94 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNi3(PO4)2 + SbPO4 + Mg2P2O7 + Ni(SbO3)2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <0 1 1> | 211.9 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 329.3 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 141.1 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 235.2 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 329.3 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 141.1 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 329.3 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 211.0 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 141.1 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 235.2 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 211.0 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 329.3 |
CdS (mp-672) | <1 1 0> | <1 1 1> | 149.5 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 235.2 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 329.3 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 211.0 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 282.3 |
Te2W (mp-22693) | <1 0 1> | <0 1 1> | 106.0 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 105.5 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 105.5 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 47.0 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 141.1 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 329.3 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 211.0 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 235.2 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 329.3 |
MoS2 (mp-1434) | <1 0 0> | <0 0 1> | 141.1 |
Al (mp-134) | <1 0 0> | <1 0 0> | 211.0 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 329.3 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 329.3 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 329.3 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 235.2 |
LiGaO2 (mp-5854) | <1 1 0> | <0 1 0> | 94.9 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 188.2 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 329.3 |
GaSe (mp-1943) | <1 1 0> | <0 0 1> | 235.2 |
GaSe (mp-1943) | <1 1 1> | <0 0 1> | 235.2 |
BN (mp-984) | <0 0 1> | <0 0 1> | 329.3 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 235.2 |
TiO2 (mp-2657) | <1 1 0> | <1 0 1> | 115.5 |
LiNbO3 (mp-3731) | <1 0 0> | <1 0 1> | 231.0 |
C (mp-66) | <1 1 0> | <0 0 1> | 329.3 |
MoS2 (mp-1434) | <0 0 1> | <0 1 1> | 106.0 |
MoS2 (mp-1434) | <1 0 1> | <0 1 0> | 284.8 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 329.3 |
KP(HO2)2 (mp-23959) | <0 0 1> | <1 0 1> | 231.0 |
KP(HO2)2 (mp-23959) | <0 1 0> | <1 0 1> | 231.0 |
LiGaO2 (mp-5854) | <0 1 1> | <0 1 1> | 211.9 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 1> | 106.0 |
CdTe (mp-406) | <1 0 0> | <0 1 1> | 211.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Mg3(PO6)2 (mp-867981) | 0.5293 | 0.555 | 3 |
Li2Cr2O7 (mp-770745) | 0.5939 | 0.068 | 3 |
Si2Sn2O7 (mp-769046) | 0.5785 | 0.086 | 3 |
Na2Mo2O7 (mp-25774) | 0.5132 | 0.000 | 3 |
Mn4(PO4)3 (mp-32010) | 0.5877 | 0.142 | 3 |
MgMo2P2O9 (mvc-10040) | 0.4386 | 0.063 | 4 |
ZnMo2P2O9 (mvc-10165) | 0.4444 | 0.027 | 4 |
ZnP2W2O9 (mvc-10178) | 0.4165 | 0.308 | 4 |
ZnBi2P2O9 (mvc-9675) | 0.3480 | 0.162 | 4 |
CaSn2P2O9 (mvc-9865) | 0.4221 | 0.093 | 4 |
Cr5O12 (mp-19575) | 0.7419 | 0.142 | 2 |
ZnCuNiP2O9 (mvc-8436) | 0.5283 | 0.113 | 5 |
CaNiSbP2O9 (mvc-8629) | 0.4899 | 0.075 | 5 |
MgNiBiP2O9 (mvc-8484) | 0.4154 | 0.141 | 5 |
SrVZn(PO4)2 (mvc-2998) | 0.5300 | 0.033 | 5 |
CaNiBiP2O9 (mvc-8742) | 0.3668 | 0.065 | 5 |
LiMnVP2(HO5)2 (mp-765378) | 0.6672 | 0.046 | 6 |
LiMnVP2(HO5)2 (mp-765074) | 0.6704 | 0.045 | 6 |
Li4MnCr2Fe3(PO4)6 (mp-779026) | 0.6647 | 1.367 | 6 |
NaCa8SmTi10(SiO5)10 (mp-705853) | 0.6637 | 0.002 | 6 |
LiMnVP2(HO5)2 (mp-765324) | 0.6667 | 0.072 | 6 |
Ca2Al2FeSi4BHO16 (mp-540713) | 0.6558 | 0.068 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesNi: 6.2 eV |
PseudopotentialsVASP PAW: Mg_pv Ni_pv Sb P O |
Final Energy/Atom-6.4703 eV |
Corrected Energy-396.2774 eV
-396.2774 eV = -362.3390 eV (uncorrected energy) - 25.2824 eV (MP Anion Correction) - 8.6560 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)