Final Magnetic Moment5.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-1.822 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.167 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.29 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToW18O49 + W8O21 + CaWO4 + Cu |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 299.4 |
LaAlO3 (mp-2920) | <1 0 0> | <1 1 1> | 146.8 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 0> | 299.4 |
LaAlO3 (mp-2920) | <1 1 0> | <1 1 0> | 254.3 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 239.6 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 59.9 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 84.8 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 299.4 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 299.4 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 169.5 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 179.7 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 169.5 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 254.3 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 179.7 |
DyScO3 (mp-31120) | <1 1 0> | <1 1 0> | 254.3 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 299.4 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 169.5 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 299.4 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 299.4 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 254.3 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 299.4 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 254.3 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 254.3 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 299.4 |
Te2Mo (mp-602) | <1 0 0> | <1 1 0> | 169.5 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 299.4 |
GaSe (mp-1943) | <0 0 1> | <1 1 0> | 254.3 |
GaSe (mp-1943) | <1 0 0> | <1 0 1> | 134.0 |
BN (mp-984) | <0 0 1> | <0 1 1> | 103.8 |
BN (mp-984) | <1 0 0> | <1 0 1> | 134.0 |
BN (mp-984) | <1 1 0> | <1 0 1> | 134.0 |
BN (mp-984) | <1 1 1> | <1 0 0> | 239.6 |
Al (mp-134) | <1 0 0> | <1 0 0> | 299.4 |
Al (mp-134) | <1 1 0> | <1 1 0> | 254.3 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 179.7 |
CdTe (mp-406) | <1 1 0> | <1 1 0> | 254.3 |
TeO2 (mp-2125) | <0 0 1> | <1 1 0> | 254.3 |
TeO2 (mp-2125) | <0 1 1> | <1 1 1> | 146.8 |
SiC (mp-7631) | <0 0 1> | <1 0 0> | 299.4 |
SiC (mp-7631) | <1 0 0> | <1 0 0> | 239.6 |
SiC (mp-7631) | <1 0 1> | <1 0 0> | 239.6 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 0> | 299.4 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 239.6 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 179.7 |
TiO2 (mp-2657) | <1 0 1> | <1 1 0> | 254.3 |
Ge3(BiO3)4 (mp-23560) | <1 0 0> | <1 0 0> | 119.8 |
Ge3(BiO3)4 (mp-23560) | <1 1 0> | <1 1 0> | 169.5 |
GdScO3 (mp-5690) | <0 0 1> | <1 1 0> | 254.3 |
GdScO3 (mp-5690) | <0 1 0> | <1 0 0> | 179.7 |
KP(HO2)2 (mp-23959) | <0 0 1> | <1 0 0> | 239.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li3CuF6 (mp-760812) | 0.2191 | 0.045 | 3 |
PrMn7O12 (mp-19354) | 0.2550 | 0.022 | 3 |
YCu7O12 (mvc-1832) | 0.2386 | 0.000 | 3 |
AlCu7O12 (mvc-1846) | 0.2774 | 0.209 | 3 |
PrMn7O12 (mp-567134) | 0.2619 | 0.022 | 3 |
MgV4(CuO4)3 (mvc-8325) | 0.1688 | 0.133 | 4 |
V4Zn(CuO4)3 (mvc-8331) | 0.1640 | 0.118 | 4 |
MgCu3(WO3)4 (mvc-8387) | 0.1478 | 0.252 | 4 |
AlV4(CuO4)3 (mvc-2181) | 0.1651 | 0.324 | 4 |
YV4(CuO4)3 (mvc-2177) | 0.1517 | 0.119 | 4 |
CaCr2Cu3(SbO6)2 (mp-510534) | 0.2075 | 0.060 | 5 |
CaNb2Ga2(CuO4)3 (mp-686705) | 0.2067 | 0.111 | 5 |
CaGa2Cu3(SbO6)2 (mp-41331) | 0.2050 | 0.080 | 5 |
NdTi3Fe(CuO4)3 (mp-690601) | 0.1841 | 0.046 | 5 |
NdTi3Fe(CuO4)3 (mp-39888) | 0.1850 | 0.046 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesW: 6.2 eV |
PseudopotentialsVASP PAW: Ca_sv Cu_pv W_pv O |
Final Energy/Atom-6.8056 eV |
Corrected Energy-162.1079 eV
Uncorrected energy = -136.1119 eV
Composition-based energy adjustment (-0.687 eV/atom x 12.0 atoms) = -8.2440 eV
Composition-based energy adjustment (-4.438 eV/atom x 4.0 atoms) = -17.7520 eV
Corrected energy = -162.1079 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)