Final Magnetic Moment0.048 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.083 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.047 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.14 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSnO + CaSiO3 + SiO2 |
Band Gap3.274 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP4/ncc [130] |
HallP 4ab 2n 1ab |
Point Group4/mmm |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 170.7 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 341.5 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 284.5 |
GaSe (mp-1943) | <1 0 0> | <1 0 1> | 133.6 |
BN (mp-984) | <0 0 1> | <0 0 1> | 284.5 |
BN (mp-984) | <1 1 0> | <1 0 1> | 133.6 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 284.5 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 227.6 |
SiC (mp-7631) | <1 0 0> | <0 0 1> | 227.6 |
SiC (mp-7631) | <1 1 0> | <1 0 0> | 241.8 |
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 284.5 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 341.5 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 170.7 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 241.8 |
AlN (mp-661) | <1 1 1> | <1 1 0> | 171.0 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 284.5 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 284.5 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 170.7 |
C (mp-66) | <1 0 0> | <0 0 1> | 113.8 |
GdScO3 (mp-5690) | <0 0 1> | <0 0 1> | 284.5 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 284.5 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 170.7 |
KP(HO2)2 (mp-23959) | <0 0 1> | <0 0 1> | 227.6 |
KP(HO2)2 (mp-23959) | <0 1 0> | <0 0 1> | 227.6 |
KP(HO2)2 (mp-23959) | <1 0 0> | <0 0 1> | 113.8 |
LaF3 (mp-905) | <1 1 0> | <0 0 1> | 284.5 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 284.5 |
GaP (mp-2490) | <1 0 0> | <0 0 1> | 284.5 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 227.6 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 227.6 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 170.7 |
BN (mp-984) | <1 0 0> | <0 0 1> | 56.9 |
BN (mp-984) | <1 0 1> | <1 0 0> | 120.9 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 284.5 |
TbScO3 (mp-31119) | <0 0 1> | <0 0 1> | 284.5 |
TbScO3 (mp-31119) | <0 1 0> | <0 0 1> | 170.7 |
Al (mp-134) | <1 0 0> | <0 0 1> | 284.5 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 284.5 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 170.7 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 0> | 241.8 |
InSb (mp-20012) | <1 0 0> | <0 0 1> | 227.6 |
BaTiO3 (mp-5986) | <0 0 1> | <0 0 1> | 284.5 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 284.5 |
SiC (mp-7631) | <1 0 1> | <0 0 1> | 227.6 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 284.5 |
Fe3O4 (mp-19306) | <1 0 0> | <0 0 1> | 284.5 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 284.5 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 284.5 |
BaTiO3 (mp-5986) | <1 1 0> | <0 0 1> | 284.5 |
NdGaO3 (mp-3196) | <0 0 1> | <0 0 1> | 284.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Si4SbO10 (mvc-8517) | 0.6983 | 0.172 | 3 |
Si4BiO10 (mvc-8520) | 0.6848 | 0.143 | 3 |
LiFe(Si2O5)2 (mp-761305) | 0.7298 | 0.086 | 4 |
MgSi4SnO10 (mvc-8457) | 0.6796 | 0.092 | 4 |
ZnSi4SnO10 (mvc-8492) | 0.6649 | 0.091 | 4 |
MgMn(Si2O5)2 (mvc-8656) | 0.7086 | 0.070 | 4 |
MnZn(Si2O5)2 (mvc-8650) | 0.7041 | 0.074 | 4 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ca_sv Si Sn_d O |
Final Energy/Atom-7.4672 eV |
Corrected Energy-505.3825 eV
Uncorrected energy = -477.9025 eV
Composition-based energy adjustment (-0.687 eV/atom x 40.0 atoms) = -27.4800 eV
Corrected energy = -505.3825 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)