Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.918 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.163 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.19 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToBiPO4 + O2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFdd2 [43] |
HallF 2 2d |
Point Groupmm2 |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 1> | <0 0 1> | 283.1 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 188.7 |
SiO2 (mp-6930) | <1 1 1> | <0 1 1> | 158.0 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 188.7 |
CdS (mp-672) | <1 1 0> | <0 1 0> | 253.5 |
YVO4 (mp-19133) | <0 0 1> | <0 1 1> | 158.0 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 94.4 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 283.1 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 283.1 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 283.1 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 94.4 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 283.1 |
Ge3(BiO3)4 (mp-23560) | <1 1 1> | <0 0 1> | 188.7 |
LaF3 (mp-905) | <1 0 1> | <0 0 1> | 283.1 |
LaF3 (mp-905) | <1 1 0> | <0 0 1> | 94.4 |
PbS (mp-21276) | <1 1 1> | <0 0 1> | 188.7 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 188.7 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 283.1 |
LaF3 (mp-905) | <0 0 1> | <0 0 1> | 94.4 |
LaF3 (mp-905) | <1 0 0> | <0 1 1> | 158.0 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 188.7 |
WS2 (mp-224) | <0 0 1> | <0 0 1> | 283.1 |
C (mp-48) | <0 0 1> | <0 1 0> | 126.7 |
WSe2 (mp-1821) | <1 0 0> | <0 1 0> | 253.5 |
WSe2 (mp-1821) | <1 1 0> | <0 1 0> | 253.5 |
ZrO2 (mp-2858) | <0 0 1> | <0 0 1> | 283.1 |
ZrO2 (mp-2858) | <1 0 0> | <0 0 1> | 283.1 |
ZrO2 (mp-2858) | <1 1 1> | <0 1 0> | 253.5 |
Ge(Bi3O5)4 (mp-23352) | <1 1 1> | <0 0 1> | 188.7 |
CaCO3 (mp-3953) | <1 0 0> | <0 1 0> | 253.5 |
YAlO3 (mp-3792) | <0 0 1> | <0 0 1> | 283.1 |
YAlO3 (mp-3792) | <0 1 0> | <0 1 1> | 158.0 |
YAlO3 (mp-3792) | <1 0 0> | <0 1 1> | 158.0 |
YAlO3 (mp-3792) | <1 1 0> | <0 0 1> | 283.1 |
YAlO3 (mp-3792) | <1 1 1> | <0 1 0> | 126.7 |
TiO2 (mp-390) | <1 0 1> | <0 1 1> | 158.0 |
ZnO (mp-2133) | <1 0 0> | <0 0 1> | 283.1 |
Cu (mp-30) | <1 0 0> | <0 1 1> | 158.0 |
LiAlO2 (mp-3427) | <1 1 0> | <0 0 1> | 94.4 |
Al2O3 (mp-1143) | <0 0 1> | <0 0 1> | 283.1 |
ZnTe (mp-2176) | <1 1 1> | <0 0 1> | 188.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
InPO4 (mp-7566) | 0.4070 | 0.000 | 3 |
CrPO4 (mp-764345) | 0.4197 | 0.023 | 3 |
CdSeO4 (mp-761036) | 0.4113 | 0.000 | 3 |
VPO4 (mp-18835) | 0.4191 | 0.000 | 3 |
SbPO5 (mvc-8677) | 0.4082 | 0.046 | 3 |
LiFe2(PO4)3 (mp-699352) | 0.3801 | 0.101 | 4 |
LiMo2(PO4)3 (mp-697773) | 0.4469 | 0.076 | 4 |
LiNi2(PO4)3 (mp-32397) | 0.3927 | 0.141 | 4 |
LiCr2(PO4)3 (mp-697765) | 0.4266 | 0.070 | 4 |
LiMn2(PO4)3 (mp-697768) | 0.4470 | 0.066 | 4 |
CrO2 (mvc-11581) | 0.6001 | 0.163 | 2 |
VO2 (mp-777469) | 0.6314 | 0.039 | 2 |
Cr5O12 (mp-19575) | 0.5552 | 0.025 | 2 |
VO2 (mvc-6918) | 0.5692 | 0.099 | 2 |
MoO2 (mvc-6944) | 0.6620 | 0.289 | 2 |
VCrP2(HO5)2 (mp-766804) | 0.5663 | 0.050 | 5 |
LiZnCr3(SO4)6 (mp-769549) | 0.6031 | 0.011 | 5 |
LiCrPO4F (mp-770575) | 0.5714 | 0.054 | 5 |
MnVP2(HO5)2 (mp-766980) | 0.5731 | 0.052 | 5 |
VFeP2(HO5)2 (mp-765969) | 0.5390 | 0.057 | 5 |
LiMgCr3Se2(SO6)4 (mp-769552) | 0.6187 | 0.002 | 6 |
Mn4Si4SnB2(HO9)2 (mp-743890) | 0.7469 | 0.000 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Bi P O |
Final Energy/Atom-6.2710 eV |
Corrected Energy-189.6339 eV
-189.6339 eV = -175.5881 eV (uncorrected energy) - 14.0458 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)