Final Magnetic Moment1.469 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.399 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.065 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.46 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNi(BiO3)2 + Ca3(PO4)2 + Ni3(PO4)2 + BiPO4 + O2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 1 0> | <1 0 1> | 124.2 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 207.7 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 207.7 |
CdS (mp-672) | <1 0 0> | <0 1 1> | 112.8 |
CdS (mp-672) | <1 1 0> | <0 1 0> | 100.1 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 311.5 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 207.7 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 207.7 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 225.6 |
BN (mp-984) | <1 0 0> | <0 0 1> | 155.8 |
BN (mp-984) | <1 1 0> | <0 0 1> | 259.6 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 207.7 |
CdTe (mp-406) | <1 0 0> | <0 1 1> | 225.5 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 259.6 |
TeO2 (mp-2125) | <0 1 1> | <0 1 1> | 225.5 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 207.7 |
SiC (mp-7631) | <1 1 0> | <1 0 1> | 248.4 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 207.7 |
LiTaO3 (mp-3666) | <1 0 0> | <0 0 1> | 207.7 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 259.6 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 207.7 |
C (mp-66) | <1 1 0> | <0 0 1> | 259.6 |
Mg (mp-153) | <1 0 0> | <1 0 1> | 248.4 |
Mg (mp-153) | <1 1 1> | <0 0 1> | 155.8 |
LaF3 (mp-905) | <1 0 1> | <0 0 1> | 207.7 |
PbS (mp-21276) | <1 1 0> | <1 1 0> | 150.8 |
GaP (mp-2490) | <1 1 0> | <0 0 1> | 207.7 |
InP (mp-20351) | <1 1 0> | <1 1 0> | 150.8 |
LaAlO3 (mp-2920) | <1 0 0> | <0 1 1> | 225.5 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 207.7 |
AlN (mp-661) | <1 1 0> | <1 0 1> | 248.4 |
InSb (mp-20012) | <1 0 0> | <0 1 1> | 225.5 |
InSb (mp-20012) | <1 1 0> | <0 0 1> | 259.6 |
PbSe (mp-2201) | <1 1 1> | <0 0 1> | 207.7 |
GaN (mp-804) | <1 0 1> | <1 0 1> | 248.4 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 155.8 |
BaTiO3 (mp-5986) | <1 0 1> | <0 0 1> | 311.5 |
BaTiO3 (mp-5986) | <1 1 0> | <0 0 1> | 207.7 |
SiO2 (mp-6930) | <1 0 0> | <1 0 1> | 248.4 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 207.7 |
NdGaO3 (mp-3196) | <0 1 0> | <0 0 1> | 207.7 |
NdGaO3 (mp-3196) | <1 0 0> | <0 0 1> | 259.6 |
NdGaO3 (mp-3196) | <1 1 1> | <0 0 1> | 259.6 |
SiC (mp-11714) | <0 0 1> | <0 0 1> | 207.7 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 225.6 |
MoSe2 (mp-1634) | <0 0 1> | <0 0 1> | 155.8 |
MoSe2 (mp-1634) | <1 0 0> | <1 0 1> | 248.4 |
Ga2O3 (mp-886) | <1 0 0> | <0 0 1> | 259.6 |
Ga2O3 (mp-886) | <1 0 1> | <1 0 0> | 225.6 |
Si (mp-149) | <1 1 0> | <1 0 1> | 124.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
La2SiO5 (mp-771045) | 0.6478 | 0.050 | 3 |
Si2Sn2O7 (mp-769046) | 0.6161 | 0.086 | 3 |
BiPO4 (mvc-9620) | 0.6176 | 0.106 | 3 |
Na2Mo2O7 (mp-25774) | 0.6209 | 0.000 | 3 |
Mn4(PO4)3 (mp-32010) | 0.6038 | 0.142 | 3 |
MgMo2P2O9 (mvc-10040) | 0.4048 | 0.063 | 4 |
CaMo2P2O9 (mvc-10055) | 0.4027 | 0.000 | 4 |
CaP2W2O9 (mvc-10157) | 0.4064 | 0.164 | 4 |
ZnP2W2O9 (mvc-10178) | 0.4039 | 0.308 | 4 |
CaSn2P2O9 (mvc-9865) | 0.4270 | 0.093 | 4 |
MgNiSbP2O9 (mvc-8327) | 0.3668 | 0.139 | 5 |
CaNiSnP2O9 (mvc-8536) | 0.5919 | 0.066 | 5 |
CaNiSbP2O9 (mvc-8629) | 0.2600 | 0.075 | 5 |
MgNiBiP2O9 (mvc-8484) | 0.5288 | 0.141 | 5 |
SrMgV(PO4)2 (mvc-2997) | 0.5765 | 0.025 | 5 |
LiMnVP2(HO5)2 (mp-765074) | 0.6688 | 0.045 | 6 |
Li4MnCr2Fe3(PO4)6 (mp-779026) | 0.6704 | 1.367 | 6 |
NaCa8SmTi10(SiO5)10 (mp-705853) | 0.6681 | 0.002 | 6 |
Li3Al3P3H2O14F (mp-695635) | 0.6314 | 0.003 | 6 |
Li4TiMn3Cr2(PO4)6 (mp-778261) | 0.6757 | 0.081 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesNi: 6.2 eV |
PseudopotentialsVASP PAW: Ca_sv Ni_pv Bi P O |
Final Energy/Atom-6.5811 eV |
Corrected Energy-402.4779 eV
-402.4779 eV = -368.5395 eV (uncorrected energy) - 25.2824 eV (MP Anion Correction) - 8.6560 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)