Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.099 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.227 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.15 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTaBiO4 + O2 |
Band Gap0.753 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 1 -1> | 275.6 |
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 215.6 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 221.2 |
AlN (mp-661) | <1 0 0> | <1 0 1> | 124.7 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 53.9 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 309.6 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 215.6 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 215.6 |
GaAs (mp-2534) | <1 1 0> | <1 0 -1> | 241.6 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 53.9 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 132.7 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 323.4 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 215.6 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 53.9 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 323.4 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 161.7 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 215.6 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 53.9 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 0> | 265.4 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 215.6 |
ZnSe (mp-1190) | <1 1 0> | <1 0 -1> | 241.6 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 309.6 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 269.5 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 269.5 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 180.2 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 -1> | 241.6 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 221.2 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 309.6 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 309.6 |
LiF (mp-1138) | <1 1 0> | <1 0 -1> | 241.6 |
Te2W (mp-22693) | <0 1 1> | <0 1 0> | 176.9 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 323.4 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 215.6 |
YVO4 (mp-19133) | <1 1 0> | <0 1 0> | 132.7 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 180.2 |
Te2Mo (mp-602) | <0 0 1> | <0 1 1> | 209.2 |
Ag (mp-124) | <1 0 0> | <1 0 -1> | 241.6 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 176.9 |
GaSe (mp-1943) | <0 0 1> | <1 1 1> | 264.7 |
BN (mp-984) | <0 0 1> | <0 1 1> | 209.2 |
BN (mp-984) | <1 0 0> | <1 1 -1> | 275.6 |
BN (mp-984) | <1 0 1> | <0 0 1> | 161.7 |
BN (mp-984) | <1 1 1> | <1 0 -1> | 241.6 |
LiNbO3 (mp-3731) | <1 1 1> | <1 0 0> | 270.3 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 -1> | 241.6 |
Bi2Se3 (mp-541837) | <1 0 0> | <1 0 -1> | 241.6 |
MoS2 (mp-1434) | <1 0 0> | <0 0 1> | 215.6 |
Al (mp-134) | <1 0 0> | <0 1 0> | 309.6 |
Al (mp-134) | <1 1 0> | <0 0 1> | 269.5 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 0> | 221.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
V2NiO6 (mp-775985) | 0.5858 | 0.091 | 3 |
Bi(TeBr2)2 (mp-29127) | 0.5251 | 0.028 | 3 |
LiFeF4 (mp-776495) | 0.6014 | 0.085 | 3 |
TaSbO4 (mp-647226) | 0.5238 | 0.203 | 3 |
CoBi2O7 (mvc-7802) | 0.5247 | 0.218 | 3 |
ErCu(WO4)2 (mp-505167) | 0.6578 | 0.035 | 4 |
InTeO3F (mp-510727) | 0.5876 | 0.000 | 4 |
HoCu(WO4)2 (mp-556266) | 0.6651 | 0.035 | 4 |
YNi(WO4)2 (mvc-680) | 0.6662 | 0.130 | 4 |
Ca2TeWO6 (mvc-6433) | 0.6031 | 0.176 | 4 |
MoN2 (mvc-13455) | 0.6707 | 0.267 | 2 |
CrN2 (mp-1096935) | 0.5117 | 0.461 | 2 |
Cr3O8 (mvc-13706) | 0.7292 | 0.347 | 2 |
Bi2O5 (mvc-8880) | 0.4721 | 0.202 | 2 |
CrN2 (mp-1015582) | 0.6952 | 0.495 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ta_pv Bi O |
Final Energy/Atom-7.3816 eV |
Corrected Energy-220.7299 eV
-220.7299 eV = -206.6841 eV (uncorrected energy) - 14.0458 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)