Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.688 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.21 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap2.199 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3c [161] |
HallR 3 2"c |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 64.9 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 324.4 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 188.1 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 194.6 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 64.9 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 324.4 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 194.6 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 194.6 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 194.6 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 64.9 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 259.5 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 259.5 |
BN (mp-984) | <1 1 0> | <0 0 1> | 64.9 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 259.5 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 194.6 |
Al (mp-134) | <1 1 1> | <0 0 1> | 194.6 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 259.5 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 129.8 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 194.6 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 324.4 |
C (mp-66) | <1 1 1> | <0 0 1> | 64.9 |
Ge3(BiO3)4 (mp-23560) | <1 1 1> | <0 0 1> | 194.6 |
LaF3 (mp-905) | <1 0 0> | <0 0 1> | 324.4 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 324.4 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 259.5 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 64.9 |
PbS (mp-21276) | <1 1 1> | <0 0 1> | 64.9 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 324.4 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 259.5 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 259.5 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 64.9 |
PbSe (mp-2201) | <1 0 0> | <0 0 1> | 194.6 |
PbSe (mp-2201) | <1 1 1> | <0 0 1> | 64.9 |
BaTiO3 (mp-5986) | <1 1 0> | <0 0 1> | 194.6 |
MoSe2 (mp-1634) | <0 0 1> | <0 0 1> | 259.5 |
SiC (mp-11714) | <0 0 1> | <0 0 1> | 259.5 |
CdSe (mp-2691) | <1 1 1> | <0 0 1> | 64.9 |
C (mp-48) | <0 0 1> | <0 0 1> | 194.6 |
WSe2 (mp-1821) | <0 0 1> | <0 0 1> | 259.5 |
CdSe (mp-2691) | <1 0 0> | <0 0 1> | 194.6 |
C (mp-48) | <1 1 0> | <1 0 1> | 199.0 |
WSe2 (mp-1821) | <1 1 0> | <0 0 1> | 259.5 |
WSe2 (mp-1821) | <1 1 1> | <0 0 1> | 259.5 |
ZrO2 (mp-2858) | <0 1 1> | <0 0 1> | 194.6 |
Ge(Bi3O5)4 (mp-23352) | <1 1 1> | <0 0 1> | 194.6 |
CaCO3 (mp-3953) | <0 0 1> | <0 0 1> | 64.9 |
CaCO3 (mp-3953) | <1 0 0> | <0 0 1> | 259.5 |
YAlO3 (mp-3792) | <1 1 0> | <0 0 1> | 324.4 |
YAlO3 (mp-3792) | <1 0 0> | <0 0 1> | 324.4 |
SiC (mp-8062) | <1 0 0> | <0 0 1> | 194.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cr2(PO4)3 (mp-540340) | 0.2019 | 0.196 | 3 |
Mo2(PO4)3 (mp-32077) | 0.2066 | 0.000 | 3 |
Cr2(PO4)3 (mp-540317) | 0.1817 | 0.071 | 3 |
Cr2(PO4)3 (mp-540211) | 0.1648 | 0.061 | 3 |
V2(PO4)3 (mp-32469) | 0.1633 | 0.015 | 3 |
CoSb3(PO4)6 (mp-775217) | 0.1141 | 0.005 | 4 |
TiSb3(PO4)6 (mp-774803) | 0.0996 | 0.020 | 4 |
Cr3Sb(PO4)6 (mp-774041) | 0.1153 | 0.051 | 4 |
V3Sb(PO4)6 (mp-772013) | 0.1096 | 0.005 | 4 |
TiTe(PO4)3 (mvc-8864) | 0.0936 | 0.021 | 4 |
Cr5O12 (mp-773920) | 0.3236 | 0.000 | 2 |
Mo4O11 (mp-622101) | 0.6530 | 0.018 | 2 |
Nb2O5 (mp-776896) | 0.5699 | 0.059 | 2 |
Mo4O11 (mp-565865) | 0.6671 | 0.026 | 2 |
V5O12 (mp-778252) | 0.3875 | 0.024 | 2 |
VCrP2(O4F)2 (mp-765139) | 0.3975 | 0.041 | 5 |
MgCr3Se2(SO6)4 (mp-769544) | 0.4893 | 0.373 | 5 |
MnVP2(O4F)2 (mp-777435) | 0.3818 | 0.002 | 5 |
MgCr3Se3(SO8)3 (mp-773999) | 0.4780 | 0.455 | 5 |
VFeP2(O4F)2 (mp-778349) | 0.4030 | 0.038 | 5 |
Zr12Si2Bi2P16PbO72 (mp-693759) | 0.6997 | 0.009 | 6 |
LiTi3MnCr(PO4)6 (mp-772224) | 0.6055 | 0.001 | 6 |
NaLiTiAl(PO4)3 (mp-776520) | 0.6949 | 0.023 | 6 |
Na2LiTi3Al(PO4)6 (mp-769074) | 0.6216 | 0.011 | 6 |
Na2LiTi3Al(PO4)6 (mp-769073) | 0.6169 | 0.014 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ti_pv Sb P O |
Final Energy/Atom-7.3473 eV |
Corrected Energy-266.6617 eV
-266.6617 eV = -249.8068 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction)
|