Final Magnetic Moment2.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.636 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.047 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.17 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCu2O3 + Mg2P2O7 + TiP2O7 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3c [161] |
HallR 3 2"c |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 64.0 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 319.8 |
GaN (mp-804) | <0 0 1> | <1 0 1> | 188.5 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 319.8 |
InAs (mp-20305) | <1 0 0> | <1 0 1> | 188.5 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 64.0 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 191.9 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 319.8 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 191.9 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 255.8 |
Al (mp-134) | <1 1 1> | <0 0 1> | 191.9 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 127.9 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 255.8 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 191.9 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 319.8 |
LaF3 (mp-905) | <0 0 1> | <0 0 1> | 191.9 |
Ge3(BiO3)4 (mp-23560) | <1 1 1> | <0 0 1> | 191.9 |
LaF3 (mp-905) | <1 0 0> | <0 0 1> | 319.8 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 319.8 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 255.8 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 319.8 |
C (mp-66) | <1 1 1> | <1 0 0> | 177.3 |
SiC (mp-11714) | <0 0 1> | <0 0 1> | 255.8 |
PbS (mp-21276) | <1 1 1> | <0 0 1> | 64.0 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 255.8 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 64.0 |
Au (mp-81) | <1 0 0> | <0 0 1> | 319.8 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 255.8 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 64.0 |
PbSe (mp-2201) | <1 0 0> | <0 0 1> | 191.9 |
PbSe (mp-2201) | <1 1 1> | <0 0 1> | 64.0 |
BaTiO3 (mp-5986) | <1 1 0> | <0 0 1> | 191.9 |
MoSe2 (mp-1634) | <0 0 1> | <0 0 1> | 255.8 |
CdSe (mp-2691) | <1 0 0> | <0 0 1> | 191.9 |
CdSe (mp-2691) | <1 1 1> | <0 0 1> | 64.0 |
CaCO3 (mp-3953) | <0 0 1> | <1 0 0> | 177.3 |
WSe2 (mp-1821) | <0 0 1> | <0 0 1> | 255.8 |
WSe2 (mp-1821) | <1 1 0> | <0 0 1> | 255.8 |
WSe2 (mp-1821) | <1 1 1> | <0 0 1> | 255.8 |
SiC (mp-8062) | <1 0 0> | <0 0 1> | 191.9 |
ZnO (mp-2133) | <1 0 0> | <0 0 1> | 319.8 |
ZrO2 (mp-2858) | <0 1 1> | <0 0 1> | 191.9 |
Ge(Bi3O5)4 (mp-23352) | <1 1 1> | <0 0 1> | 191.9 |
CaCO3 (mp-3953) | <1 0 0> | <0 0 1> | 255.8 |
YAlO3 (mp-3792) | <0 1 0> | <0 0 1> | 319.8 |
YAlO3 (mp-3792) | <1 0 0> | <0 0 1> | 319.8 |
LiAlO2 (mp-3427) | <0 0 1> | <0 0 1> | 319.8 |
SiC (mp-8062) | <1 1 0> | <0 0 1> | 319.8 |
ZnO (mp-2133) | <0 0 1> | <0 0 1> | 255.8 |
GaSb (mp-1156) | <1 0 0> | <0 0 1> | 191.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
MnPO4 (mp-773411) | 0.2422 | 0.050 | 3 |
VPO4 (mp-861584) | 0.1619 | 0.076 | 3 |
FePO4 (mp-773675) | 0.3087 | 0.045 | 3 |
TiPO4 (mp-779587) | 0.1751 | 0.077 | 3 |
TiPO4 (mp-25435) | 0.4090 | 0.087 | 3 |
VFe(PO4)2 (mp-770962) | 0.1302 | 0.019 | 4 |
TiNi(PO4)2 (mp-761309) | 0.1170 | 0.018 | 4 |
TiFe5(PO4)6 (mp-773598) | 0.1179 | 0.024 | 4 |
TiV(PO4)2 (mp-850923) | 0.1324 | 0.000 | 4 |
Ti2Ni(PO4)3 (mp-771585) | 0.1351 | 0.057 | 4 |
Mo4O11 (mp-565865) | 0.7406 | 0.005 | 2 |
VO2 (mvc-6918) | 0.7243 | 0.094 | 2 |
MoO2 (mvc-6944) | 0.6956 | 0.281 | 2 |
MgTiFe(PO4)3 (mvc-9177) | 0.0763 | 0.004 | 5 |
TiZnNi(PO4)3 (mvc-9211) | 0.0819 | 0.063 | 5 |
MgTiNi(PO4)3 (mvc-9148) | 0.0563 | 0.049 | 5 |
TiMnZn(PO4)3 (mvc-9186) | 0.0779 | 0.042 | 5 |
MgTiMn(PO4)3 (mvc-9201) | 0.0578 | 0.029 | 5 |
Na2Li3Ti3Al(PO4)6 (mp-769078) | 0.5346 | 0.065 | 6 |
NaLi3Ti2Fe2(PO4)6 (mp-850140) | 0.5661 | 0.011 | 6 |
NaLi3Ti2Cr2(PO4)6 (mp-777190) | 0.5735 | 0.020 | 6 |
LiTi3MnCr(PO4)6 (mp-772224) | 0.3162 | 0.001 | 6 |
Li2Ti2MnCr2(PO4)6 (mp-777244) | 0.4810 | 0.015 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Mg_pv Ti_pv Cu_pv P O |
Final Energy/Atom-7.1240 eV |
Corrected Energy-273.3196 eV
-273.3196 eV = -256.4646 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)