Final Magnetic Moment5.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.372 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.61 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPc [7] |
HallP 2yc |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <1 0 1> | 73.3 |
AlN (mp-661) | <1 0 0> | <1 0 1> | 220.0 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 51.8 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 149.8 |
LaAlO3 (mp-2920) | <1 1 0> | <1 0 -1> | 126.9 |
AlN (mp-661) | <1 1 0> | <1 0 -1> | 84.6 |
LaAlO3 (mp-2920) | <1 1 1> | <1 0 0> | 259.2 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 149.8 |
AlN (mp-661) | <1 0 1> | <1 0 -1> | 211.5 |
AlN (mp-661) | <1 1 1> | <1 0 -1> | 296.1 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 149.8 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 89.9 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 269.6 |
GaN (mp-804) | <1 0 1> | <1 0 -1> | 296.1 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 207.3 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 30.0 |
CeO2 (mp-20194) | <1 1 0> | <1 0 -1> | 42.3 |
CeO2 (mp-20194) | <1 1 1> | <1 0 -1> | 211.5 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 269.6 |
BaF2 (mp-1029) | <1 1 0> | <1 0 -1> | 169.2 |
SiO2 (mp-6930) | <0 0 1> | <1 0 -1> | 338.3 |
SiO2 (mp-6930) | <1 1 0> | <1 0 1> | 146.7 |
GaN (mp-804) | <1 1 0> | <1 0 -1> | 84.6 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 -1> | 126.9 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 89.9 |
SiO2 (mp-6930) | <1 0 0> | <1 0 -1> | 84.6 |
KCl (mp-23193) | <1 1 0> | <1 0 -1> | 169.2 |
InAs (mp-20305) | <1 1 0> | <1 0 -1> | 169.2 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 269.6 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 -1> | 253.8 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 209.7 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 -1> | 126.9 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 149.8 |
InAs (mp-20305) | <1 1 1> | <1 0 -1> | 338.3 |
CdS (mp-672) | <1 0 0> | <1 0 1> | 146.7 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 149.8 |
Te2W (mp-22693) | <0 1 1> | <1 0 1> | 293.4 |
CdS (mp-672) | <1 0 1> | <1 0 -1> | 296.1 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 149.8 |
LiF (mp-1138) | <1 1 0> | <1 0 -1> | 253.8 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 269.6 |
YVO4 (mp-19133) | <1 0 0> | <1 1 0> | 133.9 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 207.3 |
TePb (mp-19717) | <1 1 1> | <1 0 0> | 155.5 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 155.5 |
Te2Mo (mp-602) | <1 0 0> | <1 0 -1> | 169.2 |
Te2W (mp-22693) | <0 0 1> | <1 0 -1> | 338.3 |
Te2W (mp-22693) | <0 1 0> | <1 1 0> | 267.7 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 329.5 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 259.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
SmAlO3 (mp-7405) | 0.1643 | 0.000 | 3 |
LaGaO3 (mp-5837) | 0.2027 | 0.033 | 3 |
SrSnO3 (mp-2879) | 0.2256 | 0.000 | 3 |
SrHfO3 (mp-3378) | 0.2066 | 0.000 | 3 |
PrNiO3 (mp-25590) | 0.1473 | 0.000 | 3 |
Sr2MgUO6 (mp-972112) | 0.1846 | 0.020 | 4 |
Ca9LaMn10O30 (mp-706340) | 0.1727 | 0.055 | 4 |
Sr2UCoO6 (mp-24886) | 0.1844 | 0.192 | 4 |
CaLa(FeO3)2 (mvc-8960) | 0.0770 | 0.001 | 4 |
CaLaMn2O6 (mp-39689) | 0.0633 | 0.105 | 4 |
SrLaFeRuO6 (mp-697833) | 0.1121 | 0.032 | 5 |
CaLaFeCoO6 (mvc-8963) | 0.1189 | 0.020 | 5 |
CaLaFeCuO6 (mvc-8962) | 0.0940 | 0.045 | 5 |
CaLaMnFeO6 (mvc-16539) | 0.0549 | 0.057 | 5 |
CaLaMnFeO6 (mp-40066) | 0.0829 | 0.057 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eVNi: 6.2 eV |
PseudopotentialsVASP PAW: Ca_sv La Fe_pv Ni_pv O |
Final Energy/Atom-6.5487 eV |
Corrected Energy-149.1953 eV
-149.1953 eV = -130.9738 eV (uncorrected energy) - 9.7940 eV (MP Advanced Correction) - 8.4275 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)