Final Magnetic Moment4.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-2.437 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.247 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.89 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToFe2O3 + LaVO4 + O2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPc [7] |
HallP 2yc |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 1> | 51.4 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 151.5 |
LaAlO3 (mp-2920) | <1 1 0> | <0 1 0> | 124.5 |
AlN (mp-661) | <0 0 1> | <0 1 1> | 51.4 |
AlN (mp-661) | <1 0 0> | <1 0 -1> | 172.0 |
AlN (mp-661) | <1 1 1> | <0 1 1> | 205.5 |
CeO2 (mp-20194) | <1 1 0> | <0 1 0> | 41.5 |
CeO2 (mp-20194) | <1 1 1> | <0 1 0> | 207.5 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 90.9 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 90.9 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 242.3 |
GaN (mp-804) | <1 1 0> | <1 0 -1> | 86.0 |
GaN (mp-804) | <1 1 1> | <0 1 1> | 205.5 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 83.0 |
SiO2 (mp-6930) | <1 1 0> | <1 0 1> | 148.6 |
SiO2 (mp-6930) | <1 1 1> | <0 1 0> | 166.0 |
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 212.0 |
LaAlO3 (mp-2920) | <1 1 1> | <0 1 1> | 256.9 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 30.3 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 90.9 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 90.9 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 212.0 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 166.0 |
ZnSe (mp-1190) | <1 0 0> | <1 0 -1> | 129.0 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 90.9 |
AlN (mp-661) | <1 0 1> | <1 0 -1> | 86.0 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 83.0 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 30.3 |
GaAs (mp-2534) | <1 0 0> | <1 0 -1> | 129.0 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 166.0 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 -1> | 129.0 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 90.9 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 -1> | 215.0 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 263.0 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 332.0 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 272.6 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 263.0 |
KCl (mp-23193) | <1 1 0> | <0 1 0> | 166.0 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 0> | 207.5 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 1> | 308.3 |
Te2W (mp-22693) | <0 1 0> | <0 1 0> | 166.0 |
InAs (mp-20305) | <1 0 0> | <1 1 -1> | 298.8 |
InAs (mp-20305) | <1 1 1> | <0 1 0> | 332.0 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 290.5 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 272.6 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 249.0 |
Te2W (mp-22693) | <0 0 1> | <0 1 1> | 205.5 |
YVO4 (mp-19133) | <1 0 0> | <1 1 0> | 134.0 |
YVO4 (mp-19133) | <1 0 1> | <0 1 1> | 205.5 |
TePb (mp-19717) | <1 0 0> | <0 1 1> | 256.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Pr(CoO3)2 (mvc-12903) | 0.4612 | 0.172 | 3 |
Pr(FeO3)2 (mvc-12082) | 0.4027 | 0.182 | 3 |
PrMn2O6 (mvc-14396) | 0.3840 | 0.209 | 3 |
PrCr2O6 (mvc-14524) | 0.3998 | 0.227 | 3 |
PrTi2O6 (mvc-9263) | 0.3536 | 0.126 | 3 |
LaTiCrO6 (mvc-11948) | 0.3806 | 0.169 | 4 |
LaFeTeO6 (mvc-8907) | 0.3661 | 0.167 | 4 |
LaFeWO6 (mvc-8985) | 0.3655 | 0.079 | 4 |
LaFeMoO6 (mvc-8986) | 0.3431 | 0.120 | 4 |
LaCrFeO6 (mvc-9006) | 0.3659 | 0.241 | 4 |
CaLa2Ti2Cr2O12 (mvc-13117) | 0.5003 | 0.098 | 5 |
CaLa2Mn2(FeO6)2 (mvc-10933) | 0.5057 | 0.163 | 5 |
CaLa2Ti2Mn2O12 (mvc-14929) | 0.4764 | 0.132 | 5 |
BaNdNiSbO6 (mp-41829) | 0.5646 | 0.052 | 5 |
BaNdNiSbO6 (mp-705415) | 0.5696 | 0.052 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eVFe: 5.3 eV |
PseudopotentialsVASP PAW: La V_pv Fe_pv O |
Final Energy/Atom-7.2755 eV |
Corrected Energy-148.2168 eV
-148.2168 eV = -130.9593 eV (uncorrected energy) - 8.8300 eV (MP Advanced Correction) - 8.4275 eV (MP Anion Correction)
|