Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingAFM |
Formation Energy / Atom-3.110 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.082 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.69 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLaTaO4 + MgO + FeO |
Band Gap2.863 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPc [7] |
HallP 2yc |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 154.3 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 30.9 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 123.5 |
GaAs (mp-2534) | <1 0 0> | <0 1 0> | 131.3 |
BaF2 (mp-1029) | <1 0 0> | <1 1 -1> | 313.9 |
GaN (mp-804) | <0 0 1> | <0 1 1> | 53.5 |
GaN (mp-804) | <1 0 0> | <1 1 -1> | 251.1 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 87.5 |
LaAlO3 (mp-2920) | <1 0 0> | <0 1 1> | 214.2 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 154.3 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 109.0 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 306.3 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 123.5 |
AlN (mp-661) | <1 1 0> | <0 1 1> | 53.5 |
AlN (mp-661) | <1 1 1> | <1 1 0> | 139.8 |
CeO2 (mp-20194) | <1 1 1> | <1 1 -1> | 313.9 |
GaAs (mp-2534) | <1 1 0> | <1 0 -1> | 45.0 |
GaAs (mp-2534) | <1 1 1> | <0 1 0> | 218.8 |
GaN (mp-804) | <1 0 1> | <1 0 -1> | 225.1 |
GaN (mp-804) | <1 1 1> | <0 1 1> | 214.2 |
SiO2 (mp-6930) | <1 0 0> | <0 1 1> | 53.5 |
SiO2 (mp-6930) | <1 0 1> | <1 0 -1> | 135.1 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 92.6 |
KCl (mp-23193) | <1 0 0> | <1 1 -1> | 313.9 |
KCl (mp-23193) | <1 1 0> | <0 1 0> | 175.0 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 339.5 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 131.3 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 -1> | 45.0 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 54.5 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 109.0 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 30.9 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 0> | 43.8 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 131.3 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 92.6 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 1> | 53.5 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 -1> | 45.0 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 54.5 |
DyScO3 (mp-31120) | <1 1 0> | <1 1 -1> | 62.8 |
DyScO3 (mp-31120) | <1 1 1> | <1 1 0> | 69.9 |
InAs (mp-20305) | <1 0 0> | <1 1 -1> | 313.9 |
ZnSe (mp-1190) | <1 0 0> | <0 1 0> | 131.3 |
ZnSe (mp-1190) | <1 1 0> | <1 0 -1> | 45.0 |
ZnSe (mp-1190) | <1 1 1> | <0 1 0> | 218.8 |
Te2Mo (mp-602) | <1 0 0> | <1 1 0> | 279.6 |
Ag (mp-124) | <1 1 0> | <1 1 1> | 263.8 |
CdS (mp-672) | <1 0 0> | <1 0 1> | 228.9 |
CdS (mp-672) | <1 0 1> | <1 0 -1> | 225.1 |
CdS (mp-672) | <1 1 1> | <1 1 -1> | 251.1 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 277.8 |
LiF (mp-1138) | <1 1 1> | <1 0 -1> | 225.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
TlCoO3 (mp-770614) | 0.3329 | 0.110 | 3 |
SrBiO3 (mp-29164) | 0.3329 | 0.000 | 3 |
CaMoO3 (mvc-16572) | 0.2874 | 0.142 | 3 |
Sr5(BiO4)3 (mp-33444) | 0.3432 | 0.000 | 3 |
VCdO3 (mp-25131) | 0.3452 | 0.074 | 3 |
PrMgCr2O6 (mvc-9385) | 0.2194 | 1.325 | 4 |
PrMgV2O6 (mvc-9384) | 0.2333 | 0.141 | 4 |
PrMg(FeO3)2 (mvc-9383) | 0.2368 | 0.075 | 4 |
PrZnCr2O6 (mvc-9657) | 0.2399 | 0.147 | 4 |
LaMgCr2O6 (mvc-9858) | 0.2238 | 1.331 | 4 |
Pb3O4 (mp-636813) | 0.6600 | 0.038 | 2 |
Pb2O3 (mp-20078) | 0.7176 | 0.009 | 2 |
Al2O3 (mp-642363) | 0.6885 | 0.280 | 2 |
Mn5O8 (mp-18922) | 0.6477 | 0.009 | 2 |
Mn5O8 (mp-715008) | 0.6431 | 0.009 | 2 |
LaMgVFeO6 (mvc-8914) | 0.2194 | 0.333 | 5 |
LaMgFeWO6 (mvc-9002) | 0.1458 | 0.079 | 5 |
LaMgFeSbO6 (mvc-9012) | 0.1622 | 0.220 | 5 |
LaMgFeMoO6 (mvc-9019) | 0.2169 | 0.287 | 5 |
LaMgCrMoO6 (mvc-9867) | 0.1951 | 0.712 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: La Mg_pv Ta_pv Fe_pv O |
Final Energy/Atom-8.0706 eV |
Corrected Energy-175.3058 eV
-175.3058 eV = -161.4123 eV (uncorrected energy) - 8.4275 eV (MP Anion Correction) - 5.4660 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)