Final Magnetic Moment6.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.513 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.131 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.71 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLaVO4 + ZnO + FeO |
Band Gap0.735 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPc [7] |
HallP 2yc |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 1> | 51.6 |
LaAlO3 (mp-2920) | <1 0 0> | <0 1 0> | 208.5 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 152.2 |
LaAlO3 (mp-2920) | <1 1 0> | <0 1 0> | 125.1 |
LaAlO3 (mp-2920) | <1 1 1> | <0 1 1> | 258.1 |
AlN (mp-661) | <0 0 1> | <0 1 1> | 51.6 |
AlN (mp-661) | <1 0 0> | <1 0 -1> | 174.7 |
AlN (mp-661) | <1 0 1> | <1 0 -1> | 87.3 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 83.4 |
AlN (mp-661) | <1 1 1> | <0 1 1> | 206.5 |
CeO2 (mp-20194) | <1 0 0> | <1 1 -1> | 60.4 |
CeO2 (mp-20194) | <1 1 0> | <0 1 0> | 41.7 |
CeO2 (mp-20194) | <1 1 1> | <0 1 0> | 208.5 |
GaAs (mp-2534) | <1 0 0> | <1 0 -1> | 131.0 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 91.3 |
BaF2 (mp-1029) | <1 0 0> | <1 1 -1> | 301.9 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 166.8 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 53.1 |
GaN (mp-804) | <1 0 0> | <0 1 1> | 51.6 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 243.5 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 30.4 |
GaN (mp-804) | <1 1 1> | <0 1 1> | 206.5 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 333.5 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 83.4 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 273.9 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 91.3 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 270.1 |
KCl (mp-23193) | <1 1 0> | <0 1 0> | 166.8 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 30.4 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 213.1 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 1> | 51.6 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 91.3 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 53.1 |
DyScO3 (mp-31120) | <1 1 0> | <1 1 -1> | 60.4 |
DyScO3 (mp-31120) | <1 1 1> | <1 1 0> | 67.5 |
InAs (mp-20305) | <1 0 0> | <1 1 -1> | 301.9 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 166.8 |
InAs (mp-20305) | <1 1 1> | <0 1 0> | 333.5 |
ZnSe (mp-1190) | <1 0 0> | <1 0 -1> | 131.0 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 91.3 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 -1> | 131.0 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 91.3 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 -1> | 218.3 |
CdS (mp-672) | <0 0 1> | <1 1 1> | 256.8 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 265.5 |
CdS (mp-672) | <1 0 1> | <1 1 1> | 256.8 |
LiF (mp-1138) | <1 0 0> | <1 0 -1> | 131.0 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 91.3 |
LiF (mp-1138) | <1 1 1> | <1 0 1> | 224.2 |
Te2W (mp-22693) | <0 0 1> | <0 1 1> | 206.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li7Nb8O24 (mp-686041) | 0.5862 | 0.031 | 3 |
Ca4Nb2O9 (mp-31016) | 0.5858 | 0.000 | 3 |
Tl3Bi2I9 (mp-569203) | 0.5706 | 0.008 | 3 |
Li2MnF5 (mp-762998) | 0.5640 | 0.255 | 3 |
TiCdO3 (mp-20940) | 0.5329 | 0.040 | 3 |
PrTi2ZnO6 (mvc-9314) | 0.4743 | 0.128 | 4 |
PrMgV2O6 (mvc-9384) | 0.4984 | 0.141 | 4 |
PrMg(CoO3)2 (mvc-9403) | 0.4759 | 0.168 | 4 |
PrZn(WO3)2 (mvc-9680) | 0.4804 | 0.282 | 4 |
HoV2ZnO6 (mvc-10231) | 0.5004 | 0.082 | 4 |
Pb3O4 (mp-636813) | 0.7195 | 0.038 | 2 |
V5O9 (mp-714932) | 0.7308 | 0.017 | 2 |
Ti6O11 (mp-559964) | 0.7330 | 0.008 | 2 |
Ti4O7 (mp-12205) | 0.7324 | 0.005 | 2 |
Ti4O7 (mp-558097) | 0.7282 | 0.005 | 2 |
LiLa2Ti2CrO9 (mp-767799) | 0.4792 | 0.041 | 5 |
LaTiZnFeO6 (mvc-8970) | 0.1798 | 0.097 | 5 |
LaZnFeWO6 (mvc-9052) | 0.2847 | 0.080 | 5 |
LaZnFeMoO6 (mvc-9063) | 0.2912 | 0.079 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eVFe: 5.3 eV |
PseudopotentialsVASP PAW: La V_pv Zn Fe_pv O |
Final Energy/Atom-6.9943 eV |
Corrected Energy-157.1435 eV
-157.1435 eV = -139.8861 eV (uncorrected energy) - 8.8300 eV (MP Advanced Correction) - 8.4275 eV (MP Anion Correction)
|