Final Magnetic Moment0.909 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-3.422 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.071 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.19 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMg2TiO4 + Pr2Ti2O7 + TiO |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPmn21 [31] |
HallP 2ac 2 |
Point Groupmm2 |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 1> | 50.8 |
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 148.0 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 148.0 |
LaAlO3 (mp-2920) | <1 1 0> | <0 1 0> | 123.7 |
LaAlO3 (mp-2920) | <1 1 1> | <0 1 1> | 253.8 |
AlN (mp-661) | <0 0 1> | <0 1 1> | 50.8 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 177.6 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 212.5 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 82.4 |
AlN (mp-661) | <1 1 1> | <0 1 1> | 203.0 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 29.6 |
CeO2 (mp-20194) | <1 1 0> | <0 1 0> | 41.2 |
CeO2 (mp-20194) | <1 1 1> | <0 1 0> | 206.1 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 266.5 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 164.9 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 88.8 |
GaN (mp-804) | <1 0 0> | <0 1 1> | 50.8 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 236.9 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 29.6 |
GaN (mp-804) | <1 1 1> | <0 1 1> | 203.0 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 329.8 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 82.4 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 329.8 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 148.0 |
SiO2 (mp-6930) | <1 1 1> | <1 1 1> | 264.8 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 170.0 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 123.7 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 88.8 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 0> | 206.1 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 1> | 310.8 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 207.3 |
InAs (mp-20305) | <1 0 0> | <1 1 0> | 296.0 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 164.9 |
InAs (mp-20305) | <1 1 1> | <0 1 0> | 329.8 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 266.5 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 247.3 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 288.5 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 266.5 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 236.9 |
CdS (mp-672) | <1 0 0> | <1 0 1> | 259.0 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 266.5 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 247.3 |
Te2W (mp-22693) | <0 0 1> | <0 1 1> | 203.0 |
Te2W (mp-22693) | <0 1 0> | <0 1 0> | 164.9 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 266.5 |
YVO4 (mp-19133) | <1 0 0> | <1 1 1> | 132.4 |
YVO4 (mp-19133) | <1 0 1> | <0 1 1> | 203.0 |
TePb (mp-19717) | <1 0 0> | <0 1 1> | 253.8 |
TePb (mp-19717) | <1 1 0> | <0 1 0> | 123.7 |
TePb (mp-19717) | <1 1 1> | <0 1 1> | 152.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CaWO3 (mvc-3996) | 0.2438 | 0.123 | 3 |
CaMoO3 (mp-19012) | 0.2649 | 0.000 | 3 |
CdFeO3 (mp-777146) | 0.2504 | 0.084 | 3 |
CaMoO3 (mvc-16572) | 0.2463 | 0.134 | 3 |
NaMgF3 (mp-2955) | 0.2553 | 0.000 | 3 |
PrMgCr2O6 (mvc-9385) | 0.1390 | 0.299 | 4 |
PrMg(FeO3)2 (mvc-9383) | 0.1464 | 0.082 | 4 |
PrMgMn2O6 (mvc-9378) | 0.1397 | 0.104 | 4 |
PrZnCr2O6 (mvc-9657) | 0.1719 | 0.147 | 4 |
PrMg(NiO3)2 (mvc-9651) | 0.1814 | 0.183 | 4 |
Pb3O4 (mp-636813) | 0.6935 | 0.038 | 2 |
Al2O3 (mp-642363) | 0.7429 | 0.280 | 2 |
Mn5O8 (mp-18922) | 0.7203 | 0.009 | 2 |
Mn5O8 (mp-715008) | 0.7223 | 0.009 | 2 |
LaMgTiFeO6 (mvc-8879) | 0.1738 | 0.091 | 5 |
LaMgTiCrO6 (mvc-9835) | 0.1344 | 0.202 | 5 |
LaMgVCrO6 (mvc-9838) | 0.1833 | 0.121 | 5 |
LaMgMnCrO6 (mvc-9854) | 0.1848 | 0.209 | 5 |
LaMgCrWO6 (mvc-9857) | 0.1977 | 0.527 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Pr_3 Mg_pv Ti_pv O |
Final Energy/Atom-8.1863 eV |
Corrected Energy-171.9704 eV
Uncorrected energy = -163.7264 eV
Composition-based energy adjustment (-0.687 eV/atom x 12.0 atoms) = -8.2440 eV
Corrected energy = -171.9704 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)