Final Magnetic Moment3.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.781 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.051 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.83 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToP3(WO6)2 + MgTi4(PO4)6 + Mg3(PO4)2 + W |
Band Gap0.876 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3c [161] |
HallR 3 2"c |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 332.9 |
BaF2 (mp-1029) | <1 0 0> | <1 0 1> | 196.4 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 66.6 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 199.8 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 66.6 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 266.3 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 66.6 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 199.8 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 199.8 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 199.8 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 266.3 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 266.3 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 266.3 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 266.3 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 199.8 |
BN (mp-984) | <0 0 1> | <1 0 1> | 196.4 |
BN (mp-984) | <1 1 0> | <0 0 1> | 66.6 |
Al (mp-134) | <1 1 1> | <0 0 1> | 199.8 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 199.8 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 199.8 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 332.9 |
C (mp-66) | <1 1 0> | <0 0 1> | 266.3 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 199.8 |
Ge3(BiO3)4 (mp-23560) | <1 1 1> | <0 0 1> | 199.8 |
C (mp-66) | <1 1 1> | <0 0 1> | 66.6 |
LaF3 (mp-905) | <1 0 0> | <0 0 1> | 332.9 |
GaP (mp-2490) | <1 1 1> | <0 0 1> | 199.8 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 332.9 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 266.3 |
PbSe (mp-2201) | <1 1 0> | <0 0 1> | 266.3 |
PbSe (mp-2201) | <1 1 1> | <0 0 1> | 66.6 |
GaP (mp-2490) | <1 1 0> | <0 0 1> | 332.9 |
NdGaO3 (mp-3196) | <0 1 0> | <0 0 1> | 332.9 |
NdGaO3 (mp-3196) | <1 0 0> | <0 0 1> | 332.9 |
MoSe2 (mp-1634) | <0 0 1> | <0 0 1> | 66.6 |
MoSe2 (mp-1634) | <1 1 0> | <0 0 1> | 266.3 |
PbSe (mp-2201) | <1 0 0> | <1 0 1> | 196.4 |
Ga2O3 (mp-886) | <1 0 0> | <0 0 1> | 266.3 |
Si (mp-149) | <1 1 0> | <0 0 1> | 332.9 |
Si (mp-149) | <1 1 1> | <0 0 1> | 199.8 |
Au (mp-81) | <1 1 1> | <0 0 1> | 266.3 |
CdSe (mp-2691) | <1 0 0> | <1 0 1> | 196.4 |
CdSe (mp-2691) | <1 1 0> | <0 0 1> | 266.3 |
CdSe (mp-2691) | <1 1 1> | <0 0 1> | 66.6 |
WSe2 (mp-1821) | <0 0 1> | <0 0 1> | 66.6 |
WSe2 (mp-1821) | <1 1 0> | <0 0 1> | 266.3 |
ZrO2 (mp-2858) | <0 1 1> | <1 0 1> | 196.4 |
CaCO3 (mp-3953) | <0 0 1> | <0 0 1> | 66.6 |
SiC (mp-8062) | <1 1 0> | <0 0 1> | 332.9 |
CdWO4 (mp-19387) | <0 0 1> | <0 0 1> | 266.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
MnPO4 (mp-773411) | 0.3301 | 0.050 | 3 |
VPO4 (mp-861584) | 0.2090 | 0.076 | 3 |
FePO4 (mp-773675) | 0.3160 | 0.045 | 3 |
TiPO4 (mp-779587) | 0.2043 | 0.077 | 3 |
CrCdO4 (mp-19630) | 0.3601 | 0.012 | 3 |
TiNi(PO4)2 (mp-761309) | 0.1729 | 0.018 | 4 |
VFe(PO4)2 (mp-773926) | 0.1769 | 0.058 | 4 |
TiFe5(PO4)6 (mp-773598) | 0.1382 | 0.024 | 4 |
TiNi5(PO4)6 (mp-773434) | 0.1598 | 0.084 | 4 |
TiV(PO4)2 (mp-850923) | 0.1783 | 0.000 | 4 |
VO2 (mvc-6918) | 0.7264 | 0.094 | 2 |
MoO2 (mvc-6944) | 0.7249 | 0.281 | 2 |
Ti3MnFe2(PO4)6 (mp-776906) | 0.1488 | 0.025 | 5 |
Ti3CuNi2(PO4)6 (mp-776876) | 0.1453 | 0.038 | 5 |
MgTiMo(PO4)3 (mvc-9195) | 0.0411 | 0.001 | 5 |
TiZnMo(PO4)3 (mvc-9207) | 0.0639 | 0.010 | 5 |
TiZnP3WO12 (mvc-9230) | 0.0485 | 0.062 | 5 |
Na2Li3Ti3Al(PO4)6 (mp-769078) | 0.5273 | 0.065 | 6 |
NaLi3Ti2Fe2(PO4)6 (mp-850140) | 0.5635 | 0.011 | 6 |
NaLi3Ti2Cr2(PO4)6 (mp-777190) | 0.5932 | 0.020 | 6 |
LiTi3MnCr(PO4)6 (mp-772224) | 0.3582 | 0.001 | 6 |
Li2Ti2MnCr2(PO4)6 (mp-777244) | 0.5267 | 0.015 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesW: 6.2 eV |
PseudopotentialsVASP PAW: Mg_pv Ti_pv P W_pv O |
Final Energy/Atom-7.5190 eV |
Corrected Energy-296.2406 eV
-296.2406 eV = -270.6836 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction) - 8.7020 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)