Final Magnetic Moment35.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.503 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.297 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.59 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToY2SiO5 + V3Sb + V2O3 + Sb |
Band Gap0.326 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 1 0> | 158.4 |
KCl (mp-23193) | <1 1 1> | <0 1 0> | 211.2 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 316.9 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 142.4 |
BaF2 (mp-1029) | <1 1 1> | <0 1 0> | 211.2 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 316.9 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 142.4 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 264.0 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 0> | 211.2 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 211.2 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 264.0 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 142.4 |
LiF (mp-1138) | <1 1 1> | <0 1 0> | 316.9 |
YVO4 (mp-19133) | <1 0 1> | <0 1 0> | 211.2 |
YVO4 (mp-19133) | <1 1 0> | <0 1 0> | 316.9 |
YVO4 (mp-19133) | <1 1 1> | <0 1 0> | 264.0 |
LiNbO3 (mp-3731) | <0 0 1> | <0 1 0> | 211.2 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 264.0 |
BN (mp-984) | <0 0 1> | <0 1 0> | 211.2 |
BN (mp-984) | <1 0 1> | <0 1 0> | 158.4 |
TeO2 (mp-2125) | <1 0 0> | <0 0 1> | 142.4 |
Al (mp-134) | <1 0 0> | <0 1 0> | 264.0 |
Al (mp-134) | <1 1 0> | <0 1 0> | 211.2 |
LiGaO2 (mp-5854) | <1 0 1> | <0 1 0> | 316.9 |
SiC (mp-7631) | <0 0 1> | <0 1 0> | 264.0 |
LiTaO3 (mp-3666) | <0 0 1> | <0 1 0> | 211.2 |
TeO2 (mp-2125) | <0 0 1> | <0 1 0> | 264.0 |
TiO2 (mp-2657) | <1 0 0> | <0 1 0> | 316.9 |
TiO2 (mp-2657) | <1 1 1> | <0 1 0> | 211.2 |
GdScO3 (mp-5690) | <1 1 1> | <0 1 0> | 211.2 |
Mg (mp-153) | <1 0 0> | <0 1 0> | 316.9 |
GdScO3 (mp-5690) | <1 0 0> | <0 0 1> | 142.4 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 142.4 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 142.4 |
TbScO3 (mp-31119) | <1 0 0> | <0 0 1> | 142.4 |
TbScO3 (mp-31119) | <1 1 1> | <0 1 0> | 211.2 |
BaTiO3 (mp-5986) | <1 0 0> | <0 1 1> | 151.9 |
BaTiO3 (mp-5986) | <1 1 1> | <0 1 0> | 264.0 |
SiC (mp-11714) | <1 0 0> | <0 1 0> | 211.2 |
BaTiO3 (mp-5986) | <1 0 1> | <0 1 0> | 211.2 |
NdGaO3 (mp-3196) | <1 0 0> | <0 1 0> | 211.2 |
MoSe2 (mp-1634) | <0 0 1> | <0 1 0> | 105.6 |
SiC (mp-11714) | <0 0 1> | <0 1 0> | 264.0 |
Ga2O3 (mp-886) | <0 1 0> | <0 0 1> | 142.4 |
C (mp-48) | <1 0 0> | <0 1 0> | 211.2 |
C (mp-48) | <1 0 1> | <0 1 0> | 158.4 |
WSe2 (mp-1821) | <0 0 1> | <0 1 0> | 105.6 |
YAlO3 (mp-3792) | <0 1 0> | <0 1 0> | 158.4 |
YAlO3 (mp-3792) | <1 1 1> | <0 1 0> | 316.9 |
CdWO4 (mp-19387) | <0 0 1> | <0 1 0> | 211.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Na10Mn2O9 (mp-778825) | 0.5825 | 0.069 | 3 |
Na4NiO4 (mp-779378) | 0.6290 | 0.107 | 3 |
Zn3In2O6 (mp-682284) | 0.6617 | 0.037 | 3 |
Al5C3N (mp-570079) | 0.6540 | 0.048 | 3 |
Mg2SiO4 (mp-1020110) | 0.6410 | 0.133 | 3 |
LiVPO4 (mp-761340) | 0.5548 | 0.075 | 4 |
Li3Mn(PO4)2 (mp-31972) | 0.5965 | 0.028 | 4 |
Li3Ni(PO4)2 (mp-32398) | 0.5954 | 0.063 | 4 |
Li3V2(SiO5)2 (mp-25644) | 0.5594 | 0.064 | 4 |
Si2Ni13(SbO14)2 (mvc-9635) | 0.5940 | 0.427 | 4 |
Y4Mn13Si2(SbO14)2 (mvc-9485) | 0.3802 | 0.078 | 5 |
Y4Cr13Si2(SbO14)2 (mvc-9640) | 0.3587 | 0.270 | 5 |
Al4V13Si2(SbO14)2 (mvc-9791) | 0.4495 | 0.205 | 5 |
Y4Fe13Si2(SbO14)2 (mvc-9713) | 0.3988 | 0.656 | 5 |
Y4Ti13Si2(SbO14)2 (mvc-9261) | 0.4496 | 0.392 | 5 |
Li3MnVP2(O4F)2 (mp-763904) | 0.5778 | 0.035 | 6 |
Li3VCrP2(O4F)2 (mp-766992) | 0.6173 | 0.027 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Y_sv V_pv Si Sb O |
Final Energy/Atom-7.8112 eV |
Corrected Energy-424.2790 eV
-424.2790 eV = -382.7489 eV (uncorrected energy) - 21.8660 eV (MP Advanced Correction) - 19.6641 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)