Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.517 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.176 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.02 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToBi2O3 + ZnO |
Band Gap1.264 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3m [160] |
HallR 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 289.1 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 289.1 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 206.5 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 289.1 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 289.1 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 165.2 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 0> | 194.6 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 123.9 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 289.1 |
TeO2 (mp-2125) | <1 1 0> | <1 1 0> | 194.6 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 289.1 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 206.5 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 330.4 |
C (mp-66) | <1 1 1> | <0 0 1> | 289.1 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 165.2 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 289.1 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 289.1 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 247.8 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 112.3 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 289.1 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 289.1 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 206.5 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 194.6 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 123.9 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 165.2 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 165.2 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 165.2 |
Al (mp-134) | <1 0 0> | <1 1 0> | 194.6 |
CdTe (mp-406) | <1 1 1> | <0 0 1> | 289.1 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 165.2 |
Fe3O4 (mp-19306) | <1 1 1> | <0 0 1> | 123.9 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 123.9 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 165.2 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 206.5 |
Mg (mp-153) | <1 1 1> | <0 0 1> | 289.1 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 289.1 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 206.5 |
GaP (mp-2490) | <1 1 1> | <0 0 1> | 165.2 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 289.1 |
InP (mp-20351) | <1 1 0> | <1 1 1> | 198.9 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 123.9 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 206.5 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 289.1 |
InSb (mp-20012) | <1 1 1> | <0 0 1> | 289.1 |
BaTiO3 (mp-5986) | <0 0 1> | <0 0 1> | 330.4 |
BaTiO3 (mp-5986) | <1 0 1> | <0 0 1> | 289.1 |
MoSe2 (mp-1634) | <0 0 1> | <0 0 1> | 123.9 |
Ga2O3 (mp-886) | <0 1 0> | <0 0 1> | 289.1 |
Ga2O3 (mp-886) | <1 0 0> | <0 0 1> | 289.1 |
Au (mp-81) | <1 0 0> | <0 0 1> | 206.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
ZnCr2O4 (mvc-5335) | 0.2189 | 0.228 | 3 |
Ga3NO3 (mp-754991) | 0.2306 | 0.059 | 3 |
Mg(BiO2)2 (mvc-9584) | 0.1031 | 0.168 | 3 |
Mg(BiO2)2 (mvc-9719) | 0.1967 | 0.172 | 3 |
Co2SnO4 (mp-706412) | 0.2229 | 0.019 | 3 |
Li4Mn2OF7 (mp-767009) | 0.2115 | 0.061 | 4 |
Li4V2OF7 (mp-765046) | 0.2038 | 0.055 | 4 |
Li2V3CrO8 (mp-777666) | 0.2333 | 0.027 | 4 |
Li3Mg2Fe19O32 (mp-771996) | 0.2254 | 0.067 | 4 |
Li3Zn(Fe5O8)4 (mp-771780) | 0.2319 | 0.067 | 4 |
Fe3O4 (mp-715491) | 0.2599 | 0.015 | 2 |
Cr3N4 (mp-1014358) | 0.2745 | 0.227 | 2 |
Fe3O4 (mp-650112) | 0.2574 | 0.057 | 2 |
Fe3O4 (mp-715558) | 0.2716 | 0.076 | 2 |
Fe3O4 (mp-716052) | 0.2682 | 0.073 | 2 |
Li4Ti3Cr3(SnO8)2 (mp-776780) | 0.2310 | 0.029 | 5 |
Li4V3Cr3(FeO8)2 (mp-773698) | 0.2303 | 0.597 | 5 |
Li4V3Cr3(SnO8)2 (mp-777670) | 0.2393 | 0.000 | 5 |
Li4Ti3V2Sn3O16 (mp-777421) | 0.2368 | 0.099 | 5 |
Li4Nb3V3(SnO8)2 (mp-767976) | 0.2297 | 0.098 | 5 |
Li3MnFeCo(PO4)3 (mp-764809) | 0.6097 | 0.015 | 6 |
Li3MnFeCo(PO4)3 (mp-764869) | 0.6163 | 0.032 | 6 |
Li3MnFeCo(PO4)3 (mp-764707) | 0.6228 | 0.035 | 6 |
Li3MnFeCo(PO4)3 (mp-764969) | 0.6182 | 0.032 | 6 |
Li3MnFeCo(PO4)3 (mp-764870) | 0.6225 | 0.661 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Zn Bi O |
Final Energy/Atom-5.2349 eV |
Corrected Energy-78.9064 eV
-78.9064 eV = -73.2881 eV (uncorrected energy) - 5.6183 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)