Final Magnetic Moment0.976 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.764 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.180 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.03 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToVO2 + PrVO4 |
Band Gap0.816 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21 [4] |
HallP 2yb |
Point Group2 |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 1> | 49.5 |
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 143.2 |
LaAlO3 (mp-2920) | <1 0 1> | <0 1 1> | 148.6 |
LaAlO3 (mp-2920) | <1 1 0> | <0 1 0> | 121.3 |
LaAlO3 (mp-2920) | <1 1 1> | <0 1 1> | 247.7 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 85.9 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 171.9 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 202.1 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 80.8 |
AlN (mp-661) | <1 1 1> | <0 1 1> | 198.2 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 28.6 |
CeO2 (mp-20194) | <1 1 0> | <0 1 0> | 40.4 |
CeO2 (mp-20194) | <1 1 1> | <0 1 0> | 202.1 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 257.8 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 161.7 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 315.1 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 85.9 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 282.9 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 121.3 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 323.3 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 323.3 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 81.1 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 323.3 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 143.2 |
SiO2 (mp-6930) | <1 1 1> | <0 1 0> | 161.7 |
KCl (mp-23193) | <1 0 0> | <0 1 1> | 247.7 |
KCl (mp-23193) | <1 1 0> | <0 1 0> | 121.3 |
KCl (mp-23193) | <1 1 1> | <0 1 1> | 148.6 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 121.3 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 85.9 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 0> | 161.7 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 257.8 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 161.7 |
InAs (mp-20305) | <1 1 1> | <0 1 0> | 323.3 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 257.8 |
ZnSe (mp-1190) | <1 1 1> | <0 1 1> | 346.8 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 143.2 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 242.5 |
CdS (mp-672) | <0 0 1> | <0 1 1> | 297.2 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 343.8 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 143.2 |
Te2W (mp-22693) | <0 0 1> | <0 1 1> | 198.2 |
Te2W (mp-22693) | <0 1 0> | <0 1 0> | 161.7 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 257.8 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 315.1 |
TePb (mp-19717) | <1 0 0> | <0 1 1> | 346.8 |
TePb (mp-19717) | <1 1 0> | <0 1 0> | 121.3 |
TePb (mp-19717) | <1 1 1> | <0 1 1> | 148.6 |
Te2Mo (mp-602) | <0 0 1> | <0 1 1> | 99.1 |
Te2Mo (mp-602) | <1 0 0> | <0 1 0> | 161.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Pr(CoO3)2 (mvc-12903) | 0.3745 | 0.269 | 3 |
La8Mn7O24 (mp-766729) | 0.5112 | 0.217 | 3 |
PrMn2O6 (mvc-14396) | 0.5143 | 0.203 | 3 |
PrCr2O6 (mvc-14524) | 0.3767 | 0.232 | 3 |
Ba4Ta2O9 (mp-769344) | 0.4837 | 0.041 | 3 |
LaTiCrO6 (mvc-11948) | 0.4753 | 0.169 | 4 |
LaMnCrO6 (mvc-10014) | 0.4721 | 0.297 | 4 |
LaVCrO6 (mvc-10016) | 0.4730 | 0.318 | 4 |
LaCrFeO6 (mvc-9006) | 0.3388 | 0.242 | 4 |
LaCrNiO6 (mvc-10039) | 0.4114 | 0.279 | 4 |
Sn3F8 (mp-1443) | 0.7490 | 0.000 | 2 |
Sr8Nd2Fe5(MoO6)5 (mp-744876) | 0.5551 | 0.011 | 5 |
TiNb2Zn(PbO3)4 (mp-684723) | 0.5032 | 0.053 | 5 |
TiNb2Zn(PbO3)4 (mp-684721) | 0.5687 | 0.059 | 5 |
BaLaZnRuO6 (mp-39259) | 0.5722 | 0.029 | 5 |
BaLaMnRuO6 (mp-690567) | 0.5648 | 0.147 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Pr_3 V_pv O |
Final Energy/Atom-7.7697 eV |
Corrected Energy-155.0104 eV
-155.0104 eV = -139.8549 eV (uncorrected energy) - 8.4275 eV (MP Anion Correction) - 6.7280 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)