Final Magnetic Moment0.946 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.346 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom1.151 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.82 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMgWO4 + La2WO6 + MgO + MgCr2O4 + W |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPc [7] |
HallP 2yc |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 1> | 52.4 |
LaAlO3 (mp-2920) | <1 0 0> | <0 1 1> | 209.7 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 153.2 |
LaAlO3 (mp-2920) | <1 1 0> | <0 1 0> | 127.6 |
LaAlO3 (mp-2920) | <1 1 1> | <0 1 1> | 262.1 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 153.2 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 337.0 |
AlN (mp-661) | <1 0 1> | <1 0 -1> | 87.5 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 212.7 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 337.0 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 30.6 |
CeO2 (mp-20194) | <1 1 0> | <0 1 0> | 42.5 |
CeO2 (mp-20194) | <1 1 1> | <0 1 0> | 212.7 |
GaAs (mp-2534) | <1 0 0> | <1 0 -1> | 131.2 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 91.9 |
BaF2 (mp-1029) | <1 0 0> | <1 1 -1> | 305.1 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 170.2 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 53.0 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 265.2 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 212.7 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 85.1 |
GaN (mp-804) | <1 1 1> | <0 1 1> | 209.7 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 337.0 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 214.4 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 275.7 |
SiO2 (mp-6930) | <1 1 0> | <1 0 1> | 149.5 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 272.0 |
KCl (mp-23193) | <1 1 0> | <0 1 0> | 170.2 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 30.6 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 0> | 42.5 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 -1> | 43.7 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 53.0 |
DyScO3 (mp-31120) | <1 1 0> | <1 1 -1> | 61.0 |
DyScO3 (mp-31120) | <1 1 1> | <1 1 0> | 68.0 |
InAs (mp-20305) | <1 0 0> | <1 1 -1> | 305.1 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 170.2 |
InAs (mp-20305) | <1 1 1> | <0 1 0> | 340.4 |
ZnSe (mp-1190) | <1 0 0> | <1 0 -1> | 131.2 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 91.9 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 -1> | 131.2 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 91.9 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 -1> | 218.7 |
CdS (mp-672) | <0 0 1> | <1 1 1> | 258.1 |
CdS (mp-672) | <1 0 0> | <1 0 1> | 224.3 |
CdS (mp-672) | <1 0 1> | <1 1 1> | 258.1 |
CdS (mp-672) | <1 1 1> | <1 1 1> | 258.1 |
LiF (mp-1138) | <1 0 0> | <1 0 -1> | 131.2 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 91.9 |
LiF (mp-1138) | <1 1 1> | <1 0 -1> | 218.7 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 337.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CaWO3 (mvc-3996) | 0.2272 | 0.123 | 3 |
CaMoO3 (mp-607467) | 0.2309 | 0.000 | 3 |
CaMoO3 (mp-19012) | 0.2724 | 0.006 | 3 |
CaMoO3 (mvc-16572) | 0.2391 | 0.142 | 3 |
NaCuF3 (mp-505085) | 0.2620 | 0.019 | 3 |
PrMgTi2O6 (mvc-9086) | 0.1977 | 0.071 | 4 |
PrMgCr2O6 (mvc-9385) | 0.1881 | 1.325 | 4 |
PrMgV2O6 (mvc-9384) | 0.2002 | 0.141 | 4 |
PrMg(FeO3)2 (mvc-9383) | 0.2095 | 0.075 | 4 |
PrZnCr2O6 (mvc-9657) | 0.1907 | 0.147 | 4 |
Te8Rh3 (mp-7273) | 0.7160 | 0.000 | 2 |
Pb3O4 (mp-636813) | 0.6146 | 0.038 | 2 |
Pb2O3 (mp-20078) | 0.6769 | 0.009 | 2 |
Mn5O8 (mp-18922) | 0.6126 | 0.009 | 2 |
Mn5O8 (mp-715008) | 0.6185 | 0.009 | 2 |
LaMgFeMoO6 (mvc-9019) | 0.1026 | 0.287 | 5 |
LaMgFeSnO6 (mvc-9082) | 0.1647 | 0.293 | 5 |
LaMgCrMoO6 (mvc-9867) | 0.1690 | 0.712 | 5 |
LaMgCrSbO6 (mvc-9859) | 0.1429 | 0.842 | 5 |
LaMgCrSnO6 (mvc-9925) | 0.1227 | 0.773 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCr: 3.7 eVW: 6.2 eV |
PseudopotentialsVASP PAW: La Mg_pv Cr_pv W_pv O |
Final Energy/Atom-7.1722 eV |
Corrected Energy-164.5997 eV
-164.5997 eV = -143.4442 eV (uncorrected energy) - 12.7280 eV (MP Advanced Correction) - 8.4275 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)