Final Magnetic Moment4.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-3.144 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.699 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.43 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLa3TaO7 + LaTaO4 + MgO + MgCr2O4 + Ta |
Band Gap2.135 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPc [7] |
HallP 2yc |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 148.4 |
LaAlO3 (mp-2920) | <1 0 0> | <0 1 0> | 137.2 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 148.4 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 137.2 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 178.0 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 118.7 |
CeO2 (mp-20194) | <1 1 0> | <0 1 1> | 163.5 |
AlN (mp-661) | <1 1 0> | <0 1 1> | 54.5 |
AlN (mp-661) | <1 1 1> | <1 0 1> | 227.0 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 29.7 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 267.0 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 278.7 |
GaN (mp-804) | <1 1 1> | <1 0 -1> | 94.8 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 89.0 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 118.7 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 267.0 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 29.7 |
SiO2 (mp-6930) | <1 0 0> | <0 1 1> | 54.5 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 278.7 |
SiO2 (mp-6930) | <1 1 0> | <0 1 0> | 45.7 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 91.5 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 55.7 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 -1> | 189.6 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 89.0 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 0> | 223.0 |
InAs (mp-20305) | <1 0 0> | <0 1 0> | 228.6 |
InAs (mp-20305) | <1 1 0> | <1 1 -1> | 263.5 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 267.0 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 278.7 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 89.0 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 1> | 227.0 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 55.7 |
CdS (mp-672) | <1 0 0> | <1 0 1> | 227.0 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 237.4 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 296.7 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 267.0 |
LiF (mp-1138) | <1 1 0> | <0 1 1> | 218.0 |
Te2W (mp-22693) | <0 1 0> | <1 1 -1> | 263.5 |
Te2W (mp-22693) | <0 1 1> | <0 1 0> | 182.9 |
Te2W (mp-22693) | <0 0 1> | <1 0 1> | 227.0 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 267.0 |
YVO4 (mp-19133) | <1 0 0> | <1 0 0> | 334.5 |
YVO4 (mp-19133) | <1 1 0> | <0 1 0> | 320.1 |
YVO4 (mp-19133) | <1 1 1> | <0 1 1> | 163.5 |
Ag (mp-124) | <1 0 0> | <1 0 -1> | 142.2 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 237.4 |
Ag (mp-124) | <1 1 0> | <1 1 -1> | 197.6 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 296.7 |
GaSe (mp-1943) | <0 0 1> | <1 1 0> | 216.3 |
BN (mp-984) | <1 0 1> | <0 1 1> | 163.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ca2RuO4 (mp-21466) | 0.4938 | 0.024 | 3 |
Sr4U2O9 (mp-530539) | 0.4733 | 0.000 | 3 |
Sr5(BiO4)3 (mp-33444) | 0.4405 | 0.000 | 3 |
Na4Ge5O12 (mp-1094119) | 0.4418 | 0.158 | 3 |
Ca2RuO4 (mp-561910) | 0.4870 | 0.024 | 3 |
Zn2SnWO6 (mvc-5047) | 0.4547 | 0.137 | 4 |
Mg2SnWO6 (mvc-5015) | 0.4328 | 0.156 | 4 |
Li4Cr(WO4)3 (mp-776187) | 0.4565 | 0.180 | 4 |
Li4MnV3O12 (mp-771802) | 0.4468 | 0.148 | 4 |
Li3Ti4MnO12 (mp-771928) | 0.4471 | 0.141 | 4 |
Pb3O4 (mp-636813) | 0.5791 | 0.038 | 2 |
Pb2O3 (mp-20078) | 0.6891 | 0.009 | 2 |
Mn2O3 (mp-565203) | 0.6835 | 0.000 | 2 |
Mn5O8 (mp-18922) | 0.6659 | 0.009 | 2 |
Mn5O8 (mp-715008) | 0.6578 | 0.009 | 2 |
Li4SbTe2WO12 (mp-765930) | 0.3993 | 0.086 | 5 |
Li4VTe(WO6)2 (mp-778316) | 0.4238 | 0.056 | 5 |
CaLaTaCrO6 (mvc-10008) | 0.3346 | 0.035 | 5 |
LaMgFeSbO6 (mvc-9012) | 0.3813 | 0.220 | 5 |
LaMgFeAgO6 (mvc-8987) | 0.4110 | 0.091 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCr: 3.7 eV |
PseudopotentialsVASP PAW: La Mg_pv Ta_pv Cr_pv O |
Final Energy/Atom-8.2949 eV |
Corrected Energy-178.3510 eV
-178.3510 eV = -165.8975 eV (uncorrected energy) - 8.4275 eV (MP Anion Correction) - 4.0260 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)